TCR1-0.15
3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for TCR1-0.15 →Material demand assessment
Looking for TCR1-0.15 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
TCr1-0.15 · GB/T 5231-2012
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Copper and copper alloys
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 5231-2012
- Table / clause
- Table 2, row 17, designation C18150
- PDF page references
- 6
- Unit
- Mass fraction (wt%)
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Zr | 0.05 ~ 0.25 |
| Cr | 0.5 ~ 1.5 |
Applicability and limitations
Mass fraction wt%; GB/T 5231-2012, Table 2, row 17, designation C18150; scanned original PDF, PDF physical page 6 (printed page 5). Where Cu is marked as balance, no numerical range is invented; a dash means unspecified and is not replaced with zero. Clause 2.2: single impurity values in the table are maxima. Manufacturer supply and compliance with this standard's chemical composition require separate confirmation. Note a to Table 2 defines high-copper alloys as containing copper between 96.0% and 99.3%; this does not guarantee cold-heading wire supply. The total of table-listed impurities is ≤0.3%; this is not a maximum for each individual unlisted element.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat
Verification notes
Scanned original standard Table 2 checked manually cell by cell; continuation-table headings and footnotes b/c/d checked separately.TCr1-0.15 · GB /T 5231-2022
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Copper and copper alloys
- Subcategory
- Copper and copper alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Cr | 0.5 ~ 1.5 |
| Zr | 0.02 ~ 0.2 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
TCr1-0.15 · GB /T 5231-2022
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Copper and copper alloys
- Subcategory
- Copper and copper alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Cr | 0.5 ~ 1.5 |
| Zr | 0.02 ~ 0.2 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.