TC4
6 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for TC4 →Material demand assessment
Looking for TC4 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
TC4 · GB /T 3620.1-2007
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Titanium and titanium alloys
- Subcategory
- Titanium and titanium alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | 5.5 ~ 6.75 |
| C | ≤ 0.08 (lower limit not stated) |
| Fe | ≤ 0.3 (lower limit not stated) |
| H | ≤ 0.015 (lower limit not stated) |
| N | ≤ 0.05 (lower limit not stated) |
| O | ≤ 0.2 (lower limit not stated) |
| V | 3.5 ~ 4.5 |
| Y | ≤ 0.005 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
TC4 · GB /T 3620.1-2016
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Titanium and titanium alloys
- Subcategory
- Titanium and titanium alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | 5.5 ~ 6.75 |
| C | ≤ 0.08 (lower limit not stated) |
| Fe | ≤ 0.3 (lower limit not stated) |
| H | ≤ 0.015 (lower limit not stated) |
| N | ≤ 0.05 (lower limit not stated) |
| O | ≤ 0.2 (lower limit not stated) |
| V | 3.5 ~ 4.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
TC4 · GB /T 3621-2007
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Titanium and titanium alloys
- Subcategory
- Titanium and titanium alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | 5.5 ~ 6.75 |
| C | ≤ 0.08 (lower limit not stated) |
| Fe | ≤ 0.3 (lower limit not stated) |
| H | ≤ 0.015 (lower limit not stated) |
| N | ≤ 0.05 (lower limit not stated) |
| O | ≤ 0.2 (lower limit not stated) |
| V | 3.5 ~ 4.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
TC4 · GB /T 42159-2022
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Titanium and titanium alloys
- Subcategory
- Titanium and titanium alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | 5.5 ~ 6.75 |
| C | ≤ 0.08 (lower limit not stated) |
| Fe | ≤ 0.3 (lower limit not stated) |
| H | ≤ 0.015 (lower limit not stated) |
| N | ≤ 0.05 (lower limit not stated) |
| O | ≤ 0.2 (lower limit not stated) |
| V | 3.5 ~ 4.5 |
| Y | ≤ 0.005 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
TC4 · GJB 2219-1994
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Titanium and titanium alloys
- Subcategory
- Titanium and titanium alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | 5.5 ~ 6.75 |
| C | ≤ 0.08 (lower limit not stated) |
| Fe | ≤ 0.3 (lower limit not stated) |
| H | ≤ 0.015 (lower limit not stated) |
| N | ≤ 0.05 (lower limit not stated) |
| O | ≤ 0.2 (lower limit not stated) |
| V | 3.5 ~ 4.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
TC4 · GJB 391A-2015
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Titanium and titanium alloys
- Subcategory
- Titanium and titanium alloys
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Al | 5.5 ~ 6.75 |
| C | ≤ 0.08 (lower limit not stated) |
| Fe | ≤ 0.3 (lower limit not stated) |
| H | ≤ 0.015 (lower limit not stated) |
| N | ≤ 0.05 (lower limit not stated) |
| V | 3.5 ~ 4.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.