← BackMaterial grade directory

TAG0.15

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for TAG0.15 →

Material demand assessment

Looking for TAG0.15 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

TAg0.15 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 1, row 18, designation T11220
PDF page references
5
Unit
Mass fraction (wt%)

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Ag0.1 ~ 0.2
Bi≤ 0.002 (lower limit not stated)
Sb≤ 0.005 (lower limit not stated)
As≤ 0.01 (lower limit not stated)
Fe≤ 0.05 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Pb≤ 0.01 (lower limit not stated)
Sn≤ 0.05 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
O≤ 0.1 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; GB/T 5231-2012, Table 1, row 18, designation T11220; scanned original PDF, PDF physical page 5 (printed page 2). Dashes mean unspecified, not zero. A combined minimum must not be split into independent elemental minima. Clause 2.2: single impurity values in the table are maxima. Unlisted element limits cannot be filled with zero using another edition. Note a to Table 1: analysis of As, Bi and Sb may be omitted, but the supplier must ensure that they do not exceed the table maxima. This standard specifies only wrought copper/copper-alloy designations and chemical composition; it does not establish actual cold-heading wire supply.

Combined limits

Combined-element limits
  • Element coefficient
    Cu
    1
    Ag
    1
    Lower limit
    99.5
    Requirement
    Minimum total Cu + Ag
Elements requiring measured values from the same heat
  • Ag
  • Cu

Verification notes