← BackMaterial grade directory

TAG0.1

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for TAG0.1 →

Material demand assessment

Looking for TAG0.1 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

TAg0.1 · GB/T 5231-2001

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2001
Table / clause
Table 1 and footnotes
PDF page references
1、3、4、5、6、7、8、9、10、11、12、13、14

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Cu≥ 99.5 (upper limit not stated)
Ag0.06 ~ 0.12
Bi≤ 0.002 (lower limit not stated)
Sb≤ 0.005 (lower limit not stated)
As≤ 0.01 (lower limit not stated)
Fe≤ 0.05 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Pb≤ 0.01 (lower limit not stated)
Sn≤ 0.05 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
O≤ 0.1 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; Under 2.2, elements with specified lower and upper limits are alloying constituents; a single value is a minimum for copper and a maximum for other elements. A dash means unspecified; it is not entered as zero; Cu+Ag and Ni+Co are subject to combined ranges and are not converted into independent element ranges. The balance remains a balance; subtracting independent maxima does not establish a guaranteed range. Total impurities include all relevant impurities; The sum of listed elements is only a necessary condition and cannot replace complete impurity analysis. Product forms in the original document define the applicable wrought-product scope; they do not establish confirmed supply of cold-heading wire or final properties.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      The official GB/T 5231—2001 tables 1–4 and applicable footnotes were checked row by row against the source. The condition conflict for seven grades whose Fe content is incompatible with non-magnetic requirements is retained; it is not applied automatically.

      TAg0.1 · GB/T 5231-2012

      Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

      Material category
      Copper and copper alloys
      Material form
      Reference record
      Original record status
      Original standard verified
      Standard edition
      GB/T 5231-2012
      Table / clause
      Table 1, row 17, designation T11210
      PDF page references
      5
      Unit
      Mass fraction (wt%)

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      Cu≥ 99.5 (upper limit not stated)
      Ag0.06 ~ 0.12
      Bi≤ 0.002 (lower limit not stated)
      Sb≤ 0.005 (lower limit not stated)
      As≤ 0.01 (lower limit not stated)
      Fe≤ 0.05 (lower limit not stated)
      Ni≤ 0.2 (lower limit not stated)
      Pb≤ 0.01 (lower limit not stated)
      Sn≤ 0.05 (lower limit not stated)
      S≤ 0.01 (lower limit not stated)
      O≤ 0.1 (lower limit not stated)

      Applicability and limitations

      Mass fraction wt%; GB/T 5231-2012, Table 1, row 17, designation T11210; original scan PDF page 5 (printed page 2). A dash indicates that the value is unspecified and shall not be treated as zero; The combined lower limit shall not be split into independent lower limits for each element. Standard Clause 2.2: Impurities listed as a single value in the table are maximum limits; Limits for elements not listed cannot be supplemented as zero by referring to other versions. Table 1 Note a: As, Bi, and Sb may not be analyzed, but the supplier must guarantee that they do not exceed the upper limits listed in the table. This standard only specifies the grades and chemical compositions of wrought copper and copper alloys; actual supply of cold heading wire shall not be inferred therefrom. Table 1 Note h: This value is the copper content. Table 1 Note h: 99.5% is the lower limit for copper content, not the combined lower limit for Cu+Ag.

      Combined limits

      Combined-element limits
        Elements requiring measured values from the same heat

          Verification notes

          Each cell of Table 1 in the scanned original standard was checked manually; applicable footnotes are recorded separately.
          WhatsApp Technical enquiry →