SWRY21
2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for SWRY21 →Material demand assessment
Looking for SWRY21 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
SWRY21 · Nippon Steel Wire Rods EXE203 2008.3 / JIS G3503-2006
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- Cat. No. EXE203 2008.3 PDF; cover copyright 2008
- Document title
- Nippon Steel Wire Rods
- Table / clause
- Printed page 13, table index 2
- PDF page references
- 8
- Unit
- Mass fraction (%)
- Analysis type
- Product analysis (expressly identified in the original footnote)
- Manufacturer
- NIPPON STEEL CORPORATION
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.15 |
| Si | ≤ 0.03 (lower limit not stated) |
| Mn | 0.35 ~ 0.65 |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.023 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Historical Nippon Steel wire-rod catalogue EXE203 2008.3, PDF page 8
printed page 13, JIS G3503-2006. Product analysis (expressly identified in the original footnote). Manufacturer range data, not guaranteed standard limits or heat-specific measurements; this does not establish supply by Creation Group.
Composition conditions
- Original catalogue mass percentages, historical manufacturer data from 2008.3; Referenced standard names and editions follow the original document; this does not establish that the official texts of those standards have been obtained and verified.
- A dash or blank must not be treated as 0; only chemical composition has been checked in this batch. Mechanical properties and actual supply require separate verification under the applicable conditions.
Verification notes
Grouped tables were expanded in full and checked against original images and notes. Ordinary, residual and conditional elements are kept separate; suffix tables lacking complete base-steel composition are excluded.SWRY21 · CHINA STEEL CORPORATION · Bars and Wire Rods Product Catalogue 2014-C1 / 7.1.4 JIS G3503 (Edition unspecified)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Bars and wire rod
- Original record status
- Manufacturer source verified
- Document edition
- CAT.NO.3-BD-01-2014-C1 (stated on the back cover)
- Document title
- Bars and Wire Rods Product Catalogue
- Table / clause
- 7.1.4 JIS G3503 (Edition unspecified)
- PDF page references
- 13
- Unit
- Mass fraction (%)
- Analysis type
- The original catalogue does not explicitly identify the analysis type for this table
- Manufacturer
- CHINA STEEL CORPORATION
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.1 ~ 0.15 |
| Si | ≤ 0.03 (lower limit not stated) |
| Mn | 0.35 ~ 0.65 |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.023 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
CSC bars and wire rods catalogue CAT.NO.3-BD-01-2014-C1, PDF page 13
printed page 11; clause 7.1.4 cites JIS G3503 (edition not stated). The original catalogue does not specify the analysis type for this table. Historical manufacturer scope data; neither standard guaranteed values nor measured heat analysis, and not evidence of supply by our company.
Composition conditions
- Historical manufacturer 2014-C1 catalogue, bars/wire rod; Where the referenced standard edition is not identified, a year is not borrowed from another catalogue; a catalogue is not upgraded to the official standard text.
- A dash or blank must not be treated as zero. Composition data do not establish completeness or applicability of a formula; mechanical properties and supply require separate verification.