SWRS87A
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for SWRS87A →Material demand assessment
Looking for SWRS87A material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
SWRS87A · Nippon Steel Wire Rods EXE203 2008.3 / JIS G3502-2004
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Spring steels
- Subcategory
- Spring steels
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- Cat. No. EXE203 2008.3 PDF; cover copyright 2008
- Document title
- Nippon Steel Wire Rods
- Table / clause
- Printed page 14, table index 0
- PDF page references
- 9
- Unit
- Mass fraction (%)
- Analysis type
- The original catalogue does not explicitly identify the analysis type for this table
- Manufacturer
- NIPPON STEEL CORPORATION
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.85 ~ 0.9 |
| Si | 0.12 ~ 0.32 |
| Mn | 0.3 ~ 0.6 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Nippon Steel wire-rod catalogue EXE203 2008.3, historical material; PDF p. 9
printed p. 14; JIS G3502-2004. The original catalogue does not specify the analysis type for this table. Manufacturer range data; not a standard guarantee or a heat-lot test, and does not represent our supply.
Composition conditions
- Original catalogue mass percentages, historical manufacturer data from 2008.3; Referenced standard names and editions follow the original document; this does not establish that the official texts of those standards have been obtained and verified.
- A dash or blank must not be treated as 0; only chemical composition has been checked in this batch. Mechanical properties and actual supply require separate verification under the applicable conditions.