← BackMaterial grade directory

SWRM12K

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SWRM12K →

Material demand assessment

Looking for SWRM12K material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

SWRM12K · JIS G 3505-2017

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Mild-steel wire rod; specified killed-steel designation K
Original record status
Original standard verified
Standard edition
JIS G 3505:2017
Table / clause
Clause5/Table1 and AnnexJA.1-JA.3
PDF page references
5、6、8
Unit
Mass fraction (wt%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV:0.1500–0.2500 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1150–0.1800Known-element contribution; incomplete value; missing Si, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.1300–0.2100 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.1 ~ 0.15
Mn0.3 ~ 0.6
P≤ 0.04 (lower limit not stated)
S≤ 0.04 (lower limit not stated)

Applicability and limitations

Verify against the actual Japanese original Table 1 and normative Annex JA of JIS G3505:2017; heat analysis mass fraction wt%. The standard applies to mild steel wire rod for further processing into products such as iron wire and galvanized iron wire; electrode core wire rod is excluded.; Not automatically equivalent to special cold-heading steel. C and Mn for SWRM6/8 have only upper limits; unspecified lower limits shall not be added; Si and elements not listed in the table shall not be entered as 0; they shall not be intentionally added except for the purpose of finishing steelmaking; B addition by agreement shall follow JA.3. Add K to the end of the grade when killed steel is specified; K denotes deoxidation conditions; do not independently prescribe Al or Si content.. SWRM2/4 shall be adopted only per JA.1 agreement; SWRM17M/20M shall only have Mn changed to 0.60—0.90% per JA.2 agreement; the Mn range for ordinary 17/20 shall not be automatically expanded. When B is added per JA.3 agreement, B ≤ 70ppm, i.e., 0.007wt%; B content and B/N must be reported simultaneously. B/N for 2/4/6/8/10/12 is 0.4—1.8, and for 15/17/20/22 is 0.4—0.9. Compliance with the agreed conditions shall not be determined solely by satisfying the B upper limit; this upper limit shall not be applied if B is not agreed. The current composition table shows the default range without B addition; Agreed B/N must be verified separately in conjunction with the actual measured values of B and N for the heat; unspecified values for N shall not be entered as 0, nor shall B-suffix grades without original text basis be generated. Standard nominal diameters include 6.4mm; do not erroneously enter 6.5mm; Tolerances and diameter deviations for diameters > 25mm shall be per agreement; stricter precision per JA.4 must be separately agreed.

Verification notes

JIS G3505:2017, Table 1 and the JA low-carbon, high-manganese and deoxidation designations have been checked; Agreed addition of B requires separate verification of B/N.
WhatsApp Technical enquiry →