← BackMaterial grade directory

SWRCHB220

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SWRCHB220 →

Material demand assessment

Looking for SWRCHB220 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

SWRCHB220 · JIS G 3508-1-2005

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Boron steels
Subcategory
Boron steels
Material form
Boron-steel wire rod in an informative annex; no normative delivery guarantee
Original record status
Original standard verified
Standard edition
JIS G 3508-1:2005
Table / clause
Annex 2 (informative), Table 1
PDF page references
21
Unit
Mass fraction (wt%)
Analysis type
Reference composition table

Carbon-equivalent reference

IIW / CEV:0.2700–0.3800 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):≥ 0.2073Known-element contribution; incomplete value; missing Cu, Cr, Ni, Mo, V; B has no specified upper limit; the carbon-equivalent upper bound cannot be determined Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2300–0.3200 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.17 ~ 0.23
Si0.1 ~ 0.35
Mn0.6 ~ 0.9
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
B≥ 0.0008 (upper limit not stated)

Applicability and limitations

The actual basis is the original Japanese version of JIS G3508-1:2005; This is not a verification conclusion based on the official original text of the 2010 edition. This record covers SWRCHB feedstock wire rod.; The delivery condition, mechanical properties, and applicable standards of SWCHB wire after processing must be confirmed separately; they shall not be automatically interchanged or used to create new supply commitments. B only specifies a lower limit ≥0.0008%, and the original table has no upper limit; general boron upper limits shall not be entered; Unlisted elements shall not be filled as 0. This grade is listed only in Annex 2 (Reference) and does not belong to the 12 normative grades in Clause 3 of the main text. The appendix notes that hardenability data and actual-use records are missing.; The reference chemical table cannot be regarded as a normative delivery guarantee. The chemical table in the appendix contains only six elements: C/Si/Mn/P/S/B; The Cr/Cu/Ni limits and the B/Si remarks from Table 2 of the main text shall not be directly applied to this reference appendix. No guaranteed hardenability, tensile strength, hardness, decarburization, or default delivery specifications are provided based on this.

Verification notes

Annex 2 (informative), Table 1 in the actual original Japanese 2005 edition has been checked; Informative annex only, not a normative main-text grade designation.

SWRCHB220 · JIS G 3508-1-2010

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Boron steels
Subcategory
Boron steels
Material form
Boron-steel wire rod in an informative annex; no normative delivery guarantee
Original record status
Original standard verified
Standard edition
JIS G 3508-1:2010
Table / clause
Informative Annex JB, Table JB.1
PDF page references
20
Unit
Mass fraction (wt%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV:0.2700–0.3800 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):≥ 0.2073Known-element contribution; incomplete value; missing Cu, Cr, Ni, Mo, V; B has no specified upper limit; the carbon-equivalent upper bound cannot be determined Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2300–0.3200 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.17 ~ 0.23
Si0.1 ~ 0.35
Mn0.6 ~ 0.9
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
B≥ 0.0008 (upper limit not stated)

Applicability and limitations

Annex JB of the Japanese original version of JIS G 3508-1:2010 is for informational reference; These 12 grades have been separated from Clause 3 of the main text. ; The appendix explicitly lacks hardenability data and records of actual use; JB.1 composition cannot be used as a normative delivery guarantee. ; JB.1 only lists C, Si, Mn, P, S, B; Cu/Ni/Cr limits or B/Si agreement notes from Table 2 of the main text shall not be directly applied. ; This record does not establish suitability for a cold-heading process or a commitment to supply from stock..

Verification notes

Informative Annex JB, Table JB.1 in the original Japanese 2010 was checked row by row; Not a main-text grade designation.
WhatsApp Technical enquiry →