SWRCH6A-D
3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for SWRCH6A-D →Material demand assessment
Looking for SWRCH6A-D material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
SWRCH6A-D · Q/320582 SGGT503-2025 (Edition 0)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Cold-heading steel
- Subcategory
- Cold-heading steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- Edition 0 (2025); issued 2025-10-29; effective 2025-11-07
- Document title
- Hot-rolled cold-heading steel wire rod for automotive fasteners
- Table / clause
- Table 1
- PDF page references
- 4
- Unit
- Mass fraction (wt%)
- Manufacturer
- Jiangsu Shagang Steel Co., Ltd.
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.08 (lower limit not stated) |
| Si | ≤ 0.1 (lower limit not stated) |
| Mn | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Al | ≥ 0.02 (upper limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
| Mo | ≤ 0.05 (lower limit not stated) |
Applicability and limitations
Shagang Q/320582 SGGT503-2025 (edition 0), Table 1, row 1 (PDF page 4), cast analysis wt%; applies to the hot-rolled wire rod specified by the standard. Where Table 1 specifies otherwise, the limits in that row take precedence. Orders and actual supply require separate confirmation; this is not a supply commitment by Creation Group.
Composition conditions
- Table 1: heat analysis, mass fraction wt%; a dash is not zero, and unlisted elements must not be assumed to be zero.
- Clause 6.1.3 residual limits: Cr≤0.20%, Ni≤0.20%, Cu≤0.20%, Mo≤0.05%; where Table 1 specifies otherwise, follow the grade entry.
- Product scope: 5.0–38 mm diameter wire rod for automotive fasteners, hot rolled without twist and subjected to controlled cooling; delivery condition: hot rolled.
- Table 2: oxygen≤30×10⁻⁶ and nitrogen≤70×10⁻⁶; these are not alloy-element fields in mass fraction wt%.
- Clauses 6.8/6.9 call for reporting measured hardness and mechanical data for information only, not as delivery acceptance criteria; no generic mechanical values are entered.
Verification notes
The 2025 manufacturer document, Edition 0, Table 1 and clause 6.1.3 were checked row by row; cells obscured by the watermark were additionally checked against the rendered original page.SWRCH6A-D · Q/320582 SGY503-2024 (2nd edition)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Cold-heading steel
- Subcategory
- Cold-heading steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- Edition 2 (2024); issued 2025-02-14; effective 2025-02-18
- Document title
- Hot-rolled cold-heading steel wire rod for automotive fasteners
- Table / clause
- Table 1
- PDF page references
- 4
- Unit
- Mass fraction (wt%)
- Manufacturer
- Jiangsu Shagang Group Co., Ltd.
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.08 (lower limit not stated) |
| Si | ≤ 0.1 (lower limit not stated) |
| Mn | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Al | ≥ 0.02 (upper limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
| Mo | ≤ 0.05 (lower limit not stated) |
Applicability and limitations
Shagang Q/320582 SGY503-2024 (edition 2), Table 1, row 1 (scanned PDF page 4), cast analysis wt%; older edition implemented in month 2 of 2025, kept separate from SGGT503—2025 edition 0. Orders and supply require separate confirmation; this is not a supply commitment by Creation Group.
Composition conditions
- 2024, 2nd edition, scanned original, Table 1: heat analysis, mass fraction wt%; a dash is not zero.
- Clause 6.1.3 residual limits: Cr≤0.20%, Ni≤0.20%, Cu≤0.20%, Mo≤0.05%; where Table 1 specifies otherwise, follow the grade entry.
- In Table 1, AlT is the lower limit for total aluminium; B was a separate column in the earlier edition, while Ti, Ni, V, etc. appear in notes.
- Table 2: oxygen≤30×10⁻⁶ and nitrogen≤70×10⁻⁶; these are not alloy-element fields in mass fraction wt%.
- Scope: hot-rolled wire rod for automotive fasteners. Measured hardness and mechanical data in Clauses 6.8/6.9 are not delivery requirements; no generic properties are entered.
Verification notes
The scanned original of the 2024 Edition 2 was visually checked row by row against Table 1. Composition for grades with the same designation matches the 2025 Edition 0; the older edition does not include ML35-D or SAE1018-D.SWRCH6A-D · Q/320582 SGY503-2024 (1st edition)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Cold-heading steel
- Subcategory
- Cold-heading steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- Edition 1 (2024); issued 2024-04-26; effective 2024-05-01
- Document title
- Hot-rolled cold-heading steel wire rod for automotive fasteners
- Table / clause
- Table 1
- PDF page references
- 4
- Unit
- Mass fraction (wt%)
- Manufacturer
- Jiangsu Shagang Group Co., Ltd.
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.08 (lower limit not stated) |
| Si | ≤ 0.1 (lower limit not stated) |
| Mn | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Al | ≥ 0.02 (upper limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
| Mo | ≤ 0.05 (lower limit not stated) |
Applicability and limitations
Shagang Q/320582 SGY503-2024 (edition 1), Table 1, row 1 (PDF page 4), cast analysis wt%; original grades and values of this edition are shown independently. Orders and actual supply require separate confirmation; this is not a supply commitment by Creation Group.
Composition conditions
- 2024, 1st edition, Table 1: heat analysis, mass fraction wt%; a dash is not zero.
- Clause 6.1.3 residual limits: Cr≤0.20%, Ni≤0.20%, Cu≤0.20%, Mo≤0.05%; where Table 1 specifies otherwise, follow the grade entry.
- AlT is the lower limit for total aluminium; B has a separate column, and Ti, V, etc. are in notes; preserve grade suffixes exactly as printed in this edition.
- Table 2: oxygen≤30×10⁻⁶ and nitrogen≤70×10⁻⁶; these are not alloy-element fields in mass fraction wt%.
- Measured hardness and mechanical data in Clauses 6.10/6.11 are not delivery requirements; no generic properties are entered.