SWRCH40K-1
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for SWRCH40K-1 →Material demand assessment
Looking for SWRCH40K-1 material?
Related catalog information is available. New material and processing requirements are also welcome. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
SWRCH40K-1 · Q/BQB 517-2023
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Cold-heading steel
- Subcategory
- Cold-heading steel
- Original record status
- Original standard verified
- Standard edition
- Q/BQB 517—2023
- Table / clause
- 6.1.1/Table 1, row 76, note a
- PDF page references
- 11
- Unit
- Mass fraction (wt%)
- Analysis type
- Heat analysis
Original composition-element notation and analysis basis
- Al
- Original element symbol
- Alₜ
- Symbol extracted from the original source
- Alt
- Original table column heading
- Al t
- Subscript in the original source
- t
- Subscript explanation
- Only original table subscripts shall be retained; do not expand these into total aluminum or acid-soluble aluminum; Al without specified form shall not be directly equated
- Standard edition
- Q/BQB 517—2023
- Table / clause
- 1
- Original table item number
- 76
- PDF page references
- 11
- Unit
- Mass fraction (wt%)
- Analysis type
- Heat analysis
- Original record status
- Original column symbol verified
- Original cell
- ≥0.01
When the original analysis designations differ, or a record leaves them unspecified, comparability or a match cannot be concluded directly. Subscripts not explained by the source are not expanded here.
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.37 ~ 0.44 |
| Si | ≤ 0.1 (lower limit not stated) |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Cr | 0.3 ~ 0.45 |
| Alₜ | ≥ 0.01 (upper limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
| Mo | ≤ 0.06 (lower limit not stated) |
Applicability and limitations
Q/BQB 517—2023, official original on the Baosteel website, Table 1, row 76; cast-analysis mass fraction wt%. Table footnote a: residual Cr≤0.20, Ni≤0.20, Cu≤0.20, Mo≤0.06 wt%; where this row specifies otherwise, its requirement for that element takes precedence. Unlisted elements and special agreement requirements must not be treated as zero or assumed guarantees; permitted product-analysis deviations are governed separately by GB/T 222. Wire rod is delivered hot rolled; stricter P/S under Z1 and special surface or inclusion quality must be confirmed under normative Annex A and the contractual ordering codes. Fixed mechanical properties must not be inferred from the chemistry table.