← BackMaterial grade directory

SUS440C

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SUS440C →

SUS440C · JIS G 4308-2013

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Subcategory
Martensitic stainless steel
Material form
Hot-rolled stainless-steel wire rod
Original record status
Original standard verified
Standard edition
JIS G 4308:2013
Table / clause
Table 1 · Grade designations; Table 5 · Chemical composition / Footnotes
PDF page references
4、6
Unit
Mass fraction (%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.95 ~ 1.2
Si≤ 1.0 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
Cr16.0 ~ 18.0
Mo≤ 0.75 (lower limit not stated)

Applicability and limitations

The original Japanese edition JIS G 4308:2013, Table 5, row 10, heat-analysis mass percentages. ; The standard covers hot-rolled stainless steel wire rod; Product-analysis tolerances must be checked under JIS G 0321 and purchaser requirements; tolerances are not included in the default heat-analysis range. ; Material designation and chemical composition do not establish cold-heading suitability or a supply commitment from Creation Group; Dimensions, delivery and processing condition require separate verification. ; Original footnote: the Mo maximum has been recorded according to the table footnote.

Verification notes

The grades in original Table 1–6, the heat-analysis table and footnotes were visually checked row by row; Mo footnote c

SUS440C · JIS G 4308-1998

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Subcategory
Martensitic stainless steel
Material form
Stainless-steel wire rod
Original record status
Original standard verified
Standard edition
JIS G 4308:1998
Table / clause
Main text: Table 1 / Table 4 · Footnotes
PDF page references
1、3
Unit
Mass fraction (%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.95 ~ 1.2
Si≤ 1.0 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr16.0 ~ 18.0

Applicability and limitations

The original scanned Japanese edition JIS G 4308:1998 lists SUS440C in main-text Table 1; main-text Table 4 gives heat-analysis mass percentages. ; This edition covers stainless steel wire rod; reference suffix -WR is not a separate default grade; Standard wire diameters are in Table 6; product-analysis tolerances require separate verification under Clause 4.2. ; Table 4, footnote: Ni≤0.60% is a permitted-content condition, not a default composition. ; Table 4, footnote: Mo≤0.75% is only a permitted-addition condition. ; This does not establish cold-heading suitability, stock dimensions or a supply guarantee from Creation Group.

Verification notes

Line-by-line visual check of Table 1 and Tables 2–5 in the 1998 scanned Japanese original; footnote conditions are kept separate from the default composition.