SUS430

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SUS430 →

SUS430 · JIS G 4308-1998

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Subcategory
Ferritic stainless steel
Material form
Stainless-steel wire rod
Original record status
Original standard verified
Standard edition
JIS G 4308:1998
Table / clause
Main text: Table 1 / Table 3 · Footnotes
PDF page references
1、2
Unit
Mass fraction (%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.12 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr16.0 ~ 18.0

Applicability and limitations

The original scanned Japanese edition JIS G 4308:1998 lists SUS430 in main-text Table 1; main-text Table 3 gives heat-analysis mass percentages. ; This edition covers stainless steel wire rod; reference suffix -WR is not a separate default grade; Standard wire diameters are in Table 6; product-analysis tolerances require separate verification under Clause 4.2. ; Table 3, remark: Ni≤0.60% is a permitted-content condition, not a default composition. ; This does not establish cold-heading suitability, stock dimensions or a supply guarantee from Creation Group.

Verification notes

Line-by-line visual check of Table 1 and Tables 2–5 in the 1998 scanned Japanese original; footnote conditions are kept separate from the default composition.

SUS430 · Japanese standard (number not stated)

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Ferritic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.12 (lower limit not stated)
Cr16 ~ 18
Mn≤ 1 (lower limit not stated)
Ni≤ 0.75 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.