SUS429

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SUS429 →

SUS429 · JIS G 4305-2021

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Ferritic stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
JIS G 4305-2021
Table / clause
Table 5 · Footnotes; 5.1/5.2
PDF page references
7、9、10
Unit
Mass fraction (wt%)
Analysis type
Heat analysis, not product analysis

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.12 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Mn≤ 1 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
Cr14 ~ 16

Applicability and limitations

JIS G 4305:2021, Table 5, heat analysis, mass fraction wt%; each actual edition is retained separately. Applicable to cold-rolled stainless steel plate, sheet and strip; this does not establish suitability for delivery as cold-heading wire or guarantee cold-heading performance. 5.2 product analysis permits variations under JIS G0321, Table 5; unlisted items require agreement between the parties. These variations are not added to the heat-analysis limits in this batch. A dash indicates that no general limit is specified; it is not treated as 0. Conventional welding carbon-equivalent formulas for low-alloy steels do not apply to this stainless steel category.

Verification notes

2021 Japanese original Tables 3–7, chemical composition, footnotes and clauses 5.1/5.2 checked; sheet and strip scope retained.