2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for SUS410 →SUS410 · JIS G 4308-1998
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Subcategory
- Martensitic stainless steel
- Material form
- Stainless-steel wire rod
- Original record status
- Original standard verified
- Standard edition
- JIS G 4308:1998
- Table / clause
- Main text: Table 1 / Table 4 · Footnotes
- PDF page references
- 1、3
- Unit
- Mass fraction (%)
- Analysis type
- Heat analysis
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.15 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Mn | ≤ 1.0 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Cr | 11.5 ~ 13.0 |
Applicability and limitations
The original scanned Japanese edition JIS G 4308:1998 lists SUS410 in main-text Table 1; main-text Table 4 gives heat-analysis mass percentages. This edition covers stainless steel wire rod. Reference suffix -WR is not a separate default grade. Standard wire diameters are in Table 6; product-analysis tolerances require separate verification under Clause 4.2. Footnote to Table 4: Ni≤0.60% is a permitted-content condition and is not treated as a default composition. This does not establish cold-heading suitability, stock dimensions or a supply guarantee from Creation Group.
Verification notes
Line-by-line visual check of Table 1 and Tables 2–5 in the 1998 scanned Japanese original; footnote conditions are kept separate from the default composition.SUS410 · Japanese standard (number not stated)
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Martensitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.15 (lower limit not stated) |
| Cr | 11.5 ~ 13.5 |
| Mn | ≤ 1 (lower limit not stated) |
| Ni | ≤ 0.75 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.