← BackMaterial grade directory

SUS403

3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SUS403 →

SUS403 · JIS G 4308-2013

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Subcategory
Martensitic stainless steel
Material form
Hot-rolled stainless-steel wire rod
Original record status
Original standard verified
Standard edition
JIS G 4308:2013
Table / clause
Table 1 · Grade designations; Table 5 · Chemical composition / Footnotes
PDF page references
4、6
Unit
Mass fraction (%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.15 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
Cr11.5 ~ 13.0

Applicability and limitations

JIS G 4308:2013, Japanese original, Table 5, row 1, cast-analysis mass fraction %. The standard covers stainless-steel hot-rolled wire rod. Product-analysis deviations must be checked under JIS G 0321 and purchaser requirements; deviations must not be added to the default cast-analysis range. Grade designation and chemistry do not establish cold-heading suitability or a supply commitment by our company; dimensions, delivery and process condition require separate verification.

Verification notes

The grades in original Table 1–6, the heat-analysis table and footnotes were visually checked row by row;

SUS403 · JIS G 4308-1998

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Subcategory
Martensitic stainless steel
Material form
Stainless-steel wire rod
Original record status
Original standard verified
Standard edition
JIS G 4308:1998
Table / clause
Main text: Table 1 / Table 4 · Footnotes
PDF page references
1、3
Unit
Mass fraction (%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.15 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr11.5 ~ 13.0

Applicability and limitations

The original scanned Japanese edition JIS G 4308:1998 lists SUS403 in main-text Table 1; main-text Table 4 gives heat-analysis mass percentages. This edition covers stainless steel wire rod. Reference suffix -WR is not a separate default grade. Standard wire diameters are in Table 6; product-analysis tolerances require separate verification under Clause 4.2. Footnote to Table 4: Ni≤0.60% is a permitted-content condition and is not treated as a default composition. This does not establish cold-heading suitability, stock dimensions or a supply guarantee from Creation Group.

Verification notes

Line-by-line visual check of Table 1 and Tables 2–5 in the 1998 scanned Japanese original; footnote conditions are kept separate from the default composition.

SUS403 · JIS G 4305-2021

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
JIS G 4305-2021
Table / clause
Table 6 · Footnotes; 5.1/5.2
PDF page references
7、10
Unit
Mass fraction (wt%)
Analysis type
Heat analysis, not product analysis

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.15 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)
Mn≤ 1 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni≤ 0.6 (lower limit not stated)
Cr11.5 ~ 13

Applicability and limitations

JIS G 4305:2021, Table 6, heat analysis, mass fraction wt%; each actual edition is retained separately. Applicable to cold-rolled stainless steel plate, sheet and strip; this does not establish suitability for delivery as cold-heading wire or guarantee cold-heading performance. 5.2 product analysis permits variations under JIS G0321, Table 5; unlisted items require agreement between the parties. These variations are not added to the heat-analysis limits in this batch. A dash indicates that no general limit is specified; it is not treated as 0. Conventional welding carbon-equivalent formulas for low-alloy steels do not apply to this stainless steel category.

Verification notes

2021 Japanese original Tables 3–7, chemical composition, footnotes and clauses 5.1/5.2 checked; sheet and strip scope retained.
WhatsApp Technical enquiry →