- Material category
- Stainless steel
- Material form
- Stainless-steel wire for cold heading
- Verification status
- Original standard verified
- Standard edition
- JIS G 4315:2013
- Table / clause
- Main text Table 1, Table 2, Table 3; Main text 4.1; Appendix JA (Reference) Table JA.1—JA.3
- PDF page references
- 4、5、8
- Unit
- Mass fraction (%)
- Analysis type
- Informative-annex reference
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.15 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| Mn | ≤ 1.0 (lower limit not stated) |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Ni | ≤ 0.6 (lower limit not stated) |
| Cr | 11.5 ~ 13.0 |
Applicability and limitations
Main text Table 1: WSB temper condition of SUS403, applicable for stainless steel wire for cold-heading and cold-forging. ; Main-text Table 2: WSB applies to wire diameters 0.80–17.0 mm; Table 3 specifies mechanical properties by grade, temper condition, and wire diameter; this record does not treat the values for any one range as a guarantee for all sizes.. ; Main text, Clause 4.1: The wire rod used must meet the chemical composition requirements in Clause 5 of JIS G 4308 or JIS G 4311; the applicable material and edition must also be checked for actual orders.. ; The compositions in informative Annex JA, Tables JA.1–JA.3, are for reference only; they are not separate mandatory limits for the finished steel wire specified in the main body of this standard.; Element units are mass fraction %. ; Main text, Clause 4.1: When the order requires the threaded portion to be quenched and tempered, the manufacturer must specify C≥0.08%..