← BackMaterial grade directory

SUS316-WSB

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SUS316-WSB →

SUS316-WSB · JIS G 4315-2013

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Material form
Stainless-steel wire for cold heading
Verification status
Original standard verified
Standard edition
JIS G 4315:2013
Table / clause
Main text Table 1, Table 2, Table 3; Main text 4.1; Appendix JA (Reference) Table JA.1—JA.3
PDF page references
4、5、8
Unit
Mass fraction (%)
Analysis type
Informative-annex reference

Carbon-equivalent reference

Composition from an informative standard annex is for reference only. Normative composition and edition remain unverified; standard-range carbon equivalents and reverse matching are disabled.

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni10.0 ~ 14.0
Cr16.0 ~ 18.0
Mo2.0 ~ 3.0

Applicability and limitations

Main-text Table 1: the WSB temper for SUS316 applies to stainless steel wire for cold heading and cold forging. Main-text Table 2: WSB applies to wire diameters 0.80–17.0 mm. Mechanical properties in Table 3 are divided by grade, temper and wire diameter; no individual interval is treated as a guarantee for all sizes. Main-text Clause 4.1: the wire rod used must meet the chemical composition in Clause 5 of JIS G 4308 or JIS G 4311. Actual orders require confirmation of the corresponding material and edition. The composition in informative Annex JA, Table JA.1–JA.3, is for reference only; it is not an independent mandatory limit for finished wire in the main text of this standard. Elements are expressed as mass percent. Table 3, note a: the tensile-strength range for austenitic/ferritic B types may be extended by agreement, in which case reduction of area must be ≥55%. Default and agreed values must be kept separate.

Verification notes

The main-text Table 1/2/3 and Annex JA in the original Japanese 2013 were visually checked row by row; Annex composition is for reference only
WhatsApp Technical enquiry →