SUS305J1-WSB
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for SUS305J1-WSB →SUS305J1-WSB · JIS G 4315-2013
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Material form
- Stainless-steel wire for cold heading
- Verification status
- Original standard verified
- Standard edition
- JIS G 4315:2013
- Table / clause
- Main text Table 1, Table 2, Table 3; Main text 4.1; Appendix JA (Reference) Table JA.1—JA.3
- PDF page references
- 4、5、8
- Unit
- Mass fraction (%)
- Analysis type
- Informative-annex reference
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.08 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Ni | 11.0 ~ 13.5 |
| Cr | 16.5 ~ 19.0 |
Applicability and limitations
Main-text Table 1: the WSB temper for SUS305J1 applies to stainless steel wire for cold heading and cold forging. Main-text Table 2: WSB applies to wire diameters 0.80–17.0 mm. Mechanical properties in Table 3 are divided by grade, temper and wire diameter; no individual interval is treated as a guarantee for all sizes. Main-text Clause 4.1: the wire rod used must meet the chemical composition in Clause 5 of JIS G 4308 or JIS G 4311. Actual orders require confirmation of the corresponding material and edition. The composition in informative Annex JA, Table JA.1–JA.3, is for reference only; it is not an independent mandatory limit for finished wire in the main text of this standard. Elements are expressed as mass percent. Table 3, note a: the tensile-strength range for austenitic/ferritic B types may be extended by agreement, in which case reduction of area must be ≥55%. Default and agreed values must be kept separate.