← BackMaterial grade directory

SUS304L

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SUS304L →

SUS304L · JIS G 4308-1998

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Subcategory
Austenitic stainless steel
Material form
Stainless-steel wire rod
Original record status
Original standard verified
Standard edition
JIS G 4308:1998
Table / clause
Main text: Table 1 / Table 2 · Footnotes
PDF page references
1、2
Unit
Mass fraction (%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni9.0 ~ 13.0
Cr18.0 ~ 20.0

Applicability and limitations

JIS G 4308:1998: main-text Table 1 in the scanned Japanese original lists SUS304L; main-text Table 2 gives heat analysis, mass fraction %. This edition covers stainless steel wire. The reference suffix -WR does not create another default grade. Standard wire diameters are given in Table 6; product-analysis deviations under clause 4.2 require separate verification. Cold-heading suitability, stocked sizes and supply by our company are not automatically established.

Verification notes

Line-by-line visual check of Table 1 and Tables 2–5 in the 1998 scanned Japanese original; footnote conditions are kept separate from the default composition.

SUS304L · Japanese standard (number not stated)

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr18 ~ 20
Mn≤ 0.2 (lower limit not stated)
Ni8 ~ 12
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.