← BackMaterial grade directory

SUS304L-WSA

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SUS304L-WSA →

SUS304L-WSA · JIS G 4315-2013

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Stainless-steel wire for cold heading
Verification status
Original standard verified
Standard edition
JIS G 4315:2013
Table / clause
Main text Table 1, Table 2, Table 3; Main text 4.1; Appendix JA (Reference) Table JA.1—JA.3
PDF page references
4、5、8
Unit
Mass fraction (%)
Analysis type
Informative-annex reference

Carbon-equivalent reference

Composition from an informative standard annex is for reference only. Normative composition and edition remain unverified; standard-range carbon equivalents and reverse matching are disabled.

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni9.0 ~ 13.0
Cr18.0 ~ 20.0

Applicability and limitations

Main-text Table 1: temper WSA for SUS304L, applicable to stainless steel wire for cold heading and cold forging. Main-text Table 2: WSA applies to wire diameters 0.80–5.50 mm. Mechanical properties in Table 3 vary by grade, temper and wire diameter; no single interval is presented as a guarantee for all sizes. Main-text 4.1: the wire rod used must meet the chemical-composition requirements in clause 5 of JIS G 4308 or JIS G 4311. The actual order also requires verification of the applicable material/edition. Composition in Table JA.1–JA.3 of Annex JA (informative) is reference only, not independent mandatory limits for the finished steel wire in this standard's main text. Elemental units are mass fraction %.

Verification notes

The main-text Table 1/2/3 and Annex JA in the original Japanese 2013 were visually checked row by row; Annex composition is for reference only