← BackMaterial grade directory

SUS301-CSP-EH

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SUS301-CSP-EH →

SUS301-CSP-EH · JIS G 4313:2011

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Material form
Cold-rolled stainless spring strip
Original record status
Original standard verified
Standard edition
JIS G 4313:2011
Table / clause
Main-text Table 1—5
PDF page references
4、5
Unit
Mass fraction (%)
Analysis type
Ladle analysis

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.15 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni6.0 ~ 8.0
Cr16.0 ~ 18.0

Applicability and limitations

Table 1 of the Japanese original 2011: SUS301-CSP, with temper EH in Table 5. The hardness for that temper must not be applied to other tempers. Table 5: Vickers hardness ≥490 HV in the cold-rolled or annealed/solution-treated condition. Table 2—4 gives heat analysis, mass fraction %. Strength/elongation in Table 7 applies only when requested by the purchaser; tensile testing may be omitted for thicknesses below 0.30 mm. Values after precipitation hardening in Table 6 require assessment under the applicable treatment conditions. This standard covers cold-rolled stainless steel strip for springs; it does not establish cold-heading wire applicability, stock or supply guarantees.

Verification notes

Original Japanese Table 1—5 was visually checked row by row; Listed separately by temper
WhatsApp Technical enquiry →