10 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SUS 316 →

SUS 316 · JIS G 4305-2021

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
JIS G 4305-2021
Table / clause
Table 3 · Footnotes; 5.1/5.2
PDF page references
7、8
Unit
Mass fraction (wt%)
Analysis type
Heat analysis, not product analysis

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Mn≤ 2 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni10 ~ 14
Cr16 ~ 18
Mo2 ~ 3

Applicability and limitations

JIS G 4305:2021, Table 3, heat analysis, mass fraction wt%; each actual edition is retained separately. Applicable to cold-rolled stainless steel plate, sheet and strip; this does not establish suitability for delivery as cold-heading wire or guarantee cold-heading performance. 5.2 product analysis permits variations under JIS G0321, Table 5; unlisted items require agreement between the parties. These variations are not added to the heat-analysis limits in this batch. A dash indicates that no general limit is specified; it is not treated as 0. Conventional welding carbon-equivalent formulas for low-alloy steels do not apply to this stainless steel category.

Verification notes

2021 Japanese original Tables 3–7, chemical composition, footnotes and clauses 5.1/5.2 checked; sheet and strip scope retained.

SUS 316 · JIS G 4308-2013

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Hot-rolled stainless-steel wire rod
Original record status
Original standard verified
Standard edition
JIS G 4308:2013
Table / clause
Table 1 · Grade designations; Table 2 · Chemical composition / Footnotes
PDF page references
4、5
Unit
Mass fraction (%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni10.0 ~ 14.0
Cr16.0 ~ 18.0
Mo2.0 ~ 3.0

Applicability and limitations

JIS G 4308:2013, Japanese original, Table 2, row 14, cast-analysis mass fraction %. The standard covers stainless-steel hot-rolled wire rod. Product-analysis deviations must be checked under JIS G 0321 and purchaser requirements; deviations must not be added to the default cast-analysis range. Grade designation and chemistry do not establish cold-heading suitability or a supply commitment by our company; dimensions, delivery and process condition require separate verification.

Verification notes

The grades in original Table 1–6, the heat-analysis table and footnotes were visually checked row by row; The existing same-edition reference record retains ID and is superseded by the original standard table.

SUS 316 · JIS G 4303-2005

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A material-database match does not establish cold-heading suitability or a finished-product strength commitment; Confirmation requires the actual wire condition, reduction, heat treatment and physical testing. ; The original Japanese 2005, Table 1 confirms this bar-grade designation; Composition and property sources require separate verification under Table 2—6 and the applicable condition.

SUS 316 · JIS G 4304-2005

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

SUS 316 · JIS G 4304-2021

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

SUS 316 · JIS G 4315-2000

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

SUS 316 · JIS G 4317-2018

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

SUS 316 · JIS G 4318-2016

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

SUS 316 · JIS G 4320-2003

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

SUS 316 · Q/BQB 4302-2009

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Cr16 ~ 18
Mn≤ 2 (lower limit not stated)
Mo2 ~ 3
Ni10 ~ 14
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →