ST52-3

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for ST52-3 →

St52-3 · Q/BQB 130-2003

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Slab steels
Material form
Rough-rolled slabs for rerolling
Original record status
Original standard verified
Standard edition
Q/BQB 130—2003
Table / clause
4.1.1, Table 3 and notes 1–3
PDF page references
2、4
Unit
Mass fraction (wt%)
Analysis type
Heat analysis

Source document

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

G deoxidation method; Applies to finished plate thickness <7 mm; Al is total aluminum Al_t
IIW / CEV:0.3300–0.5033 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1967–0.3233 Known-item contribution, not a complete value; missing Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2500–0.3900 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
G deoxidation method; applicable finished plate thickness 7–<18 mm; Al is total aluminium Al_t
IIW / CEV:0.3133–0.4867 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1917–0.3183 Known-item contribution, not a complete value; missing Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2400–0.3800 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
G deoxidation method; applicable finished plate thickness 18–25.4 mm; Al is total aluminium Al_t
IIW / CEV:0.3133–0.4867 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1917–0.3183 Known-item contribution, not a complete value; missing Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2400–0.3800 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.13 ~ 0.22
Si0.2 ~ 0.55
Mn1.2 ~ 1.7
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Al≥ 0.01 (upper limit not stated)

Applicability and limitations

Q/BQB 130—2003 is a standard for slabs produced by initial rolling for subsequent rerolling. The finished plate thickness in Table 3 means the plate thickness after rerolling the slab, not slab thickness or wire diameter. Table 3 gives ladle analysis in mass fraction wt%; C = capped steel, A = aluminium-killed steel, G = aluminium-silicon-killed steel, K = silicon-killed steel. Read the applicable condition row; unlisted elements are not assumed to be zero. Note 3 to Table 3 requires slabs for thick plate (finished thickness ≥15 mm) to use G aluminium-silicon-killed steel; buyer and supplier must verify applicability of rows involving other deoxidation methods. Product-analysis tolerances for killed steel are separately governed by GB/T 222 and must not be mixed with Table 3 ladle-analysis values.

Original condition-branch records

G deoxidation method; Applies to finished plate thickness <7 mm; Al is total aluminum Al_t

ElementComposition requirement
C0.13 ~ 0.22
Si0.2 ~ 0.55
Mn1.2 ~ 1.7
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Al≥ 0.01 (upper limit not stated)
Combined limits
PDF page references in the source
2
Source table row number
29

G deoxidation method; applicable finished plate thickness 7–<18 mm; Al is total aluminium Al_t

ElementComposition requirement
C0.13 ~ 0.22
Si0.2 ~ 0.55
Mn1.1 ~ 1.6
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Al≥ 0.01 (upper limit not stated)
Nb≤ 0.04 (lower limit not stated)
Combined limits
PDF page references in the source
2
Source table row number
30

G deoxidation method; applicable finished plate thickness 18–25.4 mm; Al is total aluminium Al_t

ElementComposition requirement
C0.13 ~ 0.22
Si0.2 ~ 0.55
Mn1.1 ~ 1.6
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Al≥ 0.01 (upper limit not stated)
Nb≤ 0.04 (lower limit not stated)
Combined limits
PDF page references in the source
2
Source table row number
31

A condition branch must be selected

Yes

Verification notes

Baosteel original Table 3, merged cells and notes checked row by row; select conditions by deoxidation method and finished-product thickness.