Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- Q/BQB 130—2003
- Table / clause
- 4.1.1, Table 3 and notes 1–3
- PDF page references
- 2、4
- Unit
- Mass fraction (wt%)
- Analysis type
- Heat analysis
Carbon-equivalent reference
Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.
A deoxidation method; applicable finished plate thickness 4–<7 mm; Al is total aluminium Al_t
A deoxidation method; applicable finished plate thickness 7–<13 mm; Al is total aluminium Al_t
A deoxidation method; applicable finished plate thickness 13–<18 mm; Al is total aluminium Al_t
A deoxidation method; applicable finished plate thickness 18–25.4 mm; Al is total aluminium Al_t
Composition record (conditional branches apply; this is not an unconditional requirement)
| Element | Composition requirement |
|---|---|
| C | 0.04 ~ 0.13 |
| Si | ≤ 0.08 (lower limit not stated) |
| Mn | 0.35 ~ 0.85 |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Al | ≥ 0.01 (upper limit not stated) |
Applicability and limitations
Q/BQB 130—2003 is a standard for slabs produced by initial rolling for subsequent rerolling. The finished plate thickness in Table 3 means the plate thickness after rerolling the slab, not slab thickness or wire diameter. Table 3 gives ladle analysis in mass fraction wt%; C = capped steel, A = aluminium-killed steel, G = aluminium-silicon-killed steel, K = silicon-killed steel. Read the applicable condition row; unlisted elements are not assumed to be zero. Note 3 to Table 3 requires slabs for thick plate (finished thickness ≥15 mm) to use G aluminium-silicon-killed steel; buyer and supplier must verify applicability of rows involving other deoxidation methods. Product-analysis tolerances for killed steel are separately governed by GB/T 222 and must not be mixed with Table 3 ladle-analysis values.
Original condition-branch records
A deoxidation method; applicable finished plate thickness 4–<7 mm; Al is total aluminium Al_t
| Element | Composition requirement |
|---|---|
| C | 0.04 ~ 0.13 |
| Si | ≤ 0.08 (lower limit not stated) |
| Mn | 0.35 ~ 0.85 |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Al | ≥ 0.01 (upper limit not stated) |
- Combined limits
- PDF page references in the source
- 2
- Source table row number
- 17
A deoxidation method; applicable finished plate thickness 7–<13 mm; Al is total aluminium Al_t
| Element | Composition requirement |
|---|---|
| C | 0.04 ~ 0.13 |
| Si | ≤ 0.12 (lower limit not stated) |
| Mn | 0.55 ~ 1.05 |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Al | ≥ 0.01 (upper limit not stated) |
- Combined limits
- PDF page references in the source
- 2
- Source table row number
- 18
A deoxidation method; applicable finished plate thickness 13–<18 mm; Al is total aluminium Al_t
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.17 |
| Si | ≤ 0.12 (lower limit not stated) |
| Mn | 0.55 ~ 1.05 |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Al | ≥ 0.01 (upper limit not stated) |
- Combined limits
- PDF page references in the source
- 2
- Source table row number
- 19
A deoxidation method; applicable finished plate thickness 18–25.4 mm; Al is total aluminium Al_t
| Element | Composition requirement |
|---|---|
| C | 0.08 ~ 0.17 |
| Si | ≤ 0.12 (lower limit not stated) |
| Mn | 0.75 ~ 1.25 |
| P | ≤ 0.035 (lower limit not stated) |
| S | ≤ 0.035 (lower limit not stated) |
| Al | ≥ 0.01 (upper limit not stated) |
- Combined limits
- PDF page references in the source
- 2
- Source table row number
- 20