← BackMaterial grade directory

SS400

10 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SS400 →

SS400 · JIS G 3101-2024

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Hot-rolled structural steel
Original record status
Original standard verified
Standard edition
JIS G 3101:2024
Table / clause
Clause 5, Table 2 and table note a; Clause 1 and Clause 4, Table 1
PDF page references
5、6

Carbon-equivalent reference

IIW / CEV: cannot be calculatedKnown-element contribution; incomplete value; missing C, Mn, Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm (Ito–Bessyo): cannot be calculatedKnown-element contribution; incomplete value; missing C, Si, Mn, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET: cannot be calculatedKnown-element contribution; incomplete value; missing C, Mn, Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
P≤ 0.05 (lower limit not stated)
S≤ 0.05 (lower limit not stated)

Applicability and limitations

Clause 5, Table 2 gives heat-analysis mass percentages; Table note a permits addition as needed of elements marked “—” and unlisted alloying elements; An unspecified limit does not mean zero content. Clause 1 covers hot-rolled steel products and hot-extruded sections for general structures; cold-heading wire suitability is not established. Table 1: plate, strip, sections and bars; No separate applicable size maximum is listed for this row.

Verification notes

JIS G3101:2024, Table 2 and table note a have been checked

SS400 · Q/BQB 130-2003

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
Q/BQB 130—2003
Table / clause
4.1.1, Table 3 and notes 1–3
PDF page references
2、4
Unit
Mass fraction (wt%)
Analysis type
Heat analysis

Source document

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

C deoxidation method; applicable finished plate thickness ≤6 mm
IIW / CEV:0.2100–0.3833 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1750–0.2917 Known-item contribution, not a complete value; missing Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.1900–0.3300 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
G deoxidation method; applicable finished plate thickness ≤6 mm
IIW / CEV:0.1533–0.3267 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1313–0.2550 Known-item contribution, not a complete value; missing Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.1400–0.2800 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
A deoxidation method; applicable finished plate thickness ≤6 mm; Al is total aluminium Al_t
IIW / CEV:0.1867–0.3600 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1400–0.2567 Known-item contribution, not a complete value; missing Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.1600–0.3000 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
G deoxidation method; applicable finished plate thickness >6–16 mm
IIW / CEV:0.2033–0.3767 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1463–0.2700 Known-item contribution, not a complete value; missing Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.1700–0.3100 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
A deoxidation method; applicable finished plate thickness >6–16 mm; Al is total aluminium Al_t
IIW / CEV:0.1967–0.3867 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1150–0.2370 Known-item contribution, not a complete value; missing Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.1500–0.3000 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
G deoxidation method; applicable finished plate thickness >16–30 mm
IIW / CEV:0.2133–0.3867 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1583–0.2817 Known-item contribution, not a complete value; missing Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.1800–0.3200 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
G deoxidation method; applicable finished plate thickness >30–50 mm
IIW / CEV:0.2667–0.4400 Known-item contribution, not a complete value; missing Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.1883–0.3117 Known-item contribution, not a complete value; missing Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2200–0.3600 Known-item contribution, not a complete value; missing Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.16 ~ 0.25
Si≤ 0.05 (lower limit not stated)
Mn0.3 ~ 0.8
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)

Applicability and limitations

Q/BQB 130—2003 is a standard for slabs produced by initial rolling for subsequent rerolling. The finished plate thickness in Table 3 means the plate thickness after rerolling the slab, not slab thickness or wire diameter. Table 3 gives ladle analysis in mass fraction wt%; C = capped steel, A = aluminium-killed steel, G = aluminium-silicon-killed steel, K = silicon-killed steel. Read the applicable condition row; unlisted elements are not assumed to be zero. Note 3 to Table 3 requires slabs for thick plate (finished thickness ≥15 mm) to use G aluminium-silicon-killed steel; buyer and supplier must verify applicability of rows involving other deoxidation methods. Product-analysis tolerances for killed steel are separately governed by GB/T 222 and must not be mixed with Table 3 ladle-analysis values.

Original condition-branch records

C deoxidation method; applicable finished plate thickness ≤6 mm

ElementComposition requirement
C0.16 ~ 0.25
Si≤ 0.05 (lower limit not stated)
Mn0.3 ~ 0.8
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Combined limits
PDF page references in the source
2
Source table row number
6

G deoxidation method; applicable finished plate thickness ≤6 mm

ElementComposition requirement
C0.12 ~ 0.21
Si0.04 ~ 0.3
Mn0.2 ~ 0.7
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Combined limits
PDF page references in the source
2
Source table row number
7

A deoxidation method; applicable finished plate thickness ≤6 mm; Al is total aluminium Al_t

ElementComposition requirement
C0.12 ~ 0.21
Si≤ 0.05 (lower limit not stated)
Mn0.4 ~ 0.9
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Al≥ 0.01 (upper limit not stated)
Combined limits
PDF page references in the source
2
Source table row number
8

G deoxidation method; applicable finished plate thickness >6–16 mm

ElementComposition requirement
C0.12 ~ 0.21
Si0.04 ~ 0.3
Mn0.5 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Combined limits
PDF page references in the source
2
Source table row number
9

A deoxidation method; applicable finished plate thickness >6–16 mm; Al is total aluminium Al_t

ElementComposition requirement
C0.08 ~ 0.17
Si≤ 0.06 (lower limit not stated)
Mn0.7 ~ 1.3
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Al≥ 0.01 (upper limit not stated)
Combined limits
PDF page references in the source
2
Source table row number
10

G deoxidation method; applicable finished plate thickness >16–30 mm

ElementComposition requirement
C0.13 ~ 0.22
Si0.1 ~ 0.35
Mn0.5 ~ 1.0
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Combined limits
PDF page references in the source
2
Source table row number
11

G deoxidation method; applicable finished plate thickness >30–50 mm

ElementComposition requirement
C0.15 ~ 0.24
Si0.1 ~ 0.35
Mn0.7 ~ 1.2
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Combined limits
PDF page references in the source
2
Source table row number
12

A condition branch must be selected

Yes

Verification notes

Baosteel original Table 3, merged cells and notes checked row by row; select conditions by deoxidation method and finished-product thickness.

SS400 · JIS G 3101-2010

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Material form
Hot-rolled steel for general structures
Original record status
Original standard verified
Standard edition
JIS G 3101:2010
Table / clause
Main-text Clause 3/4, Tables 1 and 2
PDF page references
5、6
Unit
Mass fraction (wt%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV: cannot be calculatedKnown-element contribution; incomplete value; missing C, Mn, Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm (Ito–Bessyo): cannot be calculatedKnown-element contribution; incomplete value; missing C, Si, Mn, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET: cannot be calculatedKnown-element contribution; incomplete value; missing C, Mn, Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
P≤ 0.05 (lower limit not stated)
S≤ 0.05 (lower limit not stated)

Applicability and limitations

The original Japanese JIS G 3101:2010, main-text Clause 3, Table 1 lists SS400; applicable forms are plate, strip, sections, flat bars and bars. ; No additional maximum is specified in the applicable-size column of Table 1; Structural-steel product forms do not automatically establish suitability or supply as cold-heading wire. ; Main-text Clause 4, Table 2 gives heat-analysis mass fractions wt%; Only the elements already recorded for this entry are listed; the unspecified dash for C/Mn does not mean 0. ; Yield strength, tensile strength, elongation and bending in main-text Clause 5, Table 3 vary with thickness, specimen and form; no general guarantee is displayed before those conditions are structured. ; Historical 2010 is displayed separately; the 2011/2015 reference record and original 2024 record must not automatically be treated as the same edition.

Verification notes

All four rows and merged cells in the original Japanese 2010, main-text Tables 1 / 2 were visually checked

SS400 · CHINA STEEL CORPORATION · Bars and Wire Rods Product Catalogue 2014-C1 / 7.1.23 JIS G3101 (Edition unspecified)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Bars and wire rod
Original record status
Manufacturer source verified
Document edition
CAT.NO.3-BD-01-2014-C1 (stated on the back cover)
Document title
Bars and Wire Rods Product Catalogue
Table / clause
7.1.23 JIS G3101 (Edition unspecified)
PDF page references
28
Unit
Mass fraction (%)
Analysis type
The original catalogue does not explicitly identify the analysis type for this table
Manufacturer
CHINA STEEL CORPORATION

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV: cannot be calculatedKnown-element contribution; incomplete value; missing C, Mn, Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm (Ito–Bessyo): cannot be calculatedKnown-element contribution; incomplete value; missing C, Si, Mn, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET: cannot be calculatedKnown-element contribution; incomplete value; missing C, Mn, Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
P≤ 0.05 (lower limit not stated)
S≤ 0.05 (lower limit not stated)

Applicability and limitations

China Steel bar and wire-rod catalogue CAT.NO.3-BD-01-2014-C1, PDF page 28

printed page 26, 7.1.23 JIS G3101 (edition not stated). The original catalogue does not explicitly identify the analysis type for this table. Historical manufacturer range data, not guaranteed standard limits or heat-specific measurements; this does not establish supply by Creation Group. Condition: mechanical properties in this table vary with diameter and specimen; Only composition is recorded in this batch; mechanical-property conditions are not flattened.

Composition conditions

Verification notes

Merged cells in all 28 catalogue tables were reconstructed geometrically, with no missing cells. Original images, continuation pages and notes are recorded; disputed conditions are withheld.

SS400 · JIS G 3101-2011

Original-source verification is incomplete; this is not a formal standard reference

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
P≤ 0.05 (lower limit not stated)
S≤ 0.05 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

SS400 · JIS G 3101-2011

Original-source verification is incomplete; this is not a formal standard reference

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
P≤ 0.05 (lower limit not stated)
S≤ 0.05 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

SS400 · JIS G 3101-2015

Original-source verification is incomplete; this is not a formal standard reference

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
P≤ 0.05 (lower limit not stated)
S≤ 0.05 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

SS400 · KS D 3503-2008

Original-source verification is incomplete; this is not a formal standard reference

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
P≤ 0.05 (lower limit not stated)
S≤ 0.05 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

SS400 · Q/ASB 271-2017

Original-source verification is incomplete; this is not a formal standard reference

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C≤ 0.2 (lower limit not stated)
Cr≤ 0.3 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)
Mn≤ 1.4 (lower limit not stated)
N≤ 0.008 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
P≤ 0.035 (lower limit not stated)
S≤ 0.035 (lower limit not stated)
Si≤ 0.35 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

SS400 · Q/BQB 303-2018

Original-source verification is incomplete; this is not a formal standard reference

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C≤ 0.21 (lower limit not stated)
Mn≤ 1.4 (lower limit not stated)
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Si≤ 0.3 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →