SNi1066 · GB /T 15620-2008

Original-source verification is incomplete; this is not a formal standard reference

Material category
Nickel and nickel alloys
Subcategory
Nickel and nickel alloys
Material form
Reference record
Verification status
Reference data; original source not verified
Classification basis (does not replace original-source composition verification)

The titles of the listed standards are nickel and nickel alloy electrodes, welding wires, forgings, or sheet and strip materials; Only the classification field is corrected; the verification status of the original chemical composition text remains unchanged.

GB/T15620-2008 Nickel and nickel alloy welding wires

GB/T13814-2008 Nickel and nickel alloy electrodes

GB/T26030-2010 Nickel and nickel alloy forgings

DIN17750:2002 Bänder und Bleche aus Nickel und Nickel-Knetlegierungen

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.02 (lower limit not stated)
Co≤ 1 (lower limit not stated)
Cr≤ 1 (lower limit not stated)
Cu≤ 0.5 (lower limit not stated)
Fe≤ 2 (lower limit not stated)
Mn≤ 1 (lower limit not stated)
Mo26 ~ 30
Ni≥ 64 (upper limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.1 (lower limit not stated)
W≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.