← BackMaterial grade directory

SMN433H2RCH

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SMN433H2RCH →

SMn433H2RCH · JIS G 3509-1-2021

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Low-alloy steel wire rod for cold heading; special hardenability designation by agreement under JA.1
Original record status
Original standard verified
Standard edition
JIS G 3509-1:2021
Table / clause
Clause4/Table1; Clause6/Table2 including residual Cu note; AnnexJA.1, conditional designation inherits HRCH chemistry
PDF page references
6、7、8、36、37、38
Unit
Mass fraction (wt%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV:0.4817–0.7250Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3525–0.4858Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4050–0.5537Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.29 ~ 0.36
Si0.15 ~ 0.35
Mn1.15 ~ 1.55
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Cr≤ 0.35 (lower limit not stated)
Cu≤ 0.3 (lower limit not stated)

Applicability and limitations

Based on Table 1/2 of the official Japanese original version of JIS G3509-1:2021, heat analysis mass fraction wt%; This record covers feedstock wire rod; it does not automatically establish the delivery properties or supply of processed WCH wire.. Ordinary RCH, hardenability-guaranteed HRCH, and agreed H1/H2 shall be recorded separately; Chemical ranges for H-class shall follow independent rows in this edition and shall not be automatically widened based on ordinary compositions. Cu≤0.30% for all grades in the table; Do not enter 0 for Mo marked with a dash or for unlisted elements; they must not be intentionally added except as needed to finish steelmaking.; Al addition for grain refinement shall be by agreement. Si is 0.15—0.35% by default; lower limits below 0.15% are adopted by agreement only; This record retains the default range; agreed Si values require separate verification against the actual specified values.. Product analysis deviations shall be verified separately according to the referenced JIS G0321 Table 4; heat limits shall not be treated as product analysis limits. Clause 7.1 applies only when specified by the purchaser. Average ferritic/total decarburized-layer depths: d≤15mm, ≤0.02/0.12mm; 15<d≤25mm, ≤0.02/0.15mm; 25<d≤32mm, ≤0.02/0.20mm; 32<d≤40mm, ≤0.03/0.25mm; 40<d≤50mm, ≤0.03/0.30mm; d>50mm, subject to agreement.. Clause 7.2: Non-metallic inclusion requirements apply only when specified by the purchaser. Use Table 4 of this edition and the corresponding JIS G0555 cleanliness methods; do not automatically equate these with ASTM E45.. Default surface defect depth ≤ 0.10mm; Stricter surface and dimensional accuracy shall be per agreement. This grade is a special hardenability mark that must be adopted by agreement in the normative annex JA.1; H1 denotes the upper 75% of the corresponding HRCH band, and H2 the lower 75%; these are neither heating-process identifiers nor fixed delivery hardness values.. Chemical composition shall adopt Table 2 of the corresponding HRCH of this edition; The original-table upper and lower hardenability limits at each distance have been verified and incorporated; use them under the actual agreed conditions. Composition alone does not establish an H1/H2 guarantee.

Verification notes

The separate composition row and Cu table note in official Japanese Table 2 (2021) have been verified. The JA.1 designation is agreement-based and inherits the corresponding HRCH chemistry. The original hardenability values at each distance have been entered; apply them only under the stated, actually agreed conditions.

Jominy end-quench hardenability (conditional requirements)

JIS G3509-1:2021 · JIS G3509-1:2021 original Japanese text · JA.1, 7.3, 9.2.3 and Table 9 · PDF pages 9, 11, 12, 15, 36

H2RCH additional hardenability band by agreement (JA.1; must be agreed in the order)

End-quench test condition temperature 870 (tolerance not listed in source document) °C; Specimen normalizing temperature 900.0 °C (tolerance not stated in the source); This is not a production heat-treatment recommendation.

Distance from quenched end (mm)Lower limit (HRC)Upper limit (HRC)
1.55055
34653
53448
72643
92337
112032
13Unspecified; do not treat as 029
15Unspecified; do not treat as 026
20Unspecified; do not treat as 023
25Unspecified; do not treat as 021
30Unspecified; do not treat as 020
35Unspecified; do not treat as 0Unspecified; do not treat as 0
40Unspecified; do not treat as 0Unspecified; do not treat as 0
45Unspecified; do not treat as 0Unspecified; do not treat as 0
50Unspecified; do not treat as 0Unspecified; do not treat as 0
WhatsApp Technical enquiry →