← BackMaterial grade directory

SGDB

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SGDB →

SGDB · Nippon Steel Wire Rods EXE203 2008.3 / JIS G3108-2004

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Carbon steel
Subcategory
Carbon steel
Material form
Wire rod
Original record status
Manufacturer source verified
Document edition
Cat. No. EXE203 2008.3 PDF; cover copyright 2008
Document title
Nippon Steel Wire Rods
Table / clause
Printed page 14, table index 2
PDF page references
9
Unit
Mass fraction (%)
Analysis type
Heat analysis (identified as ladle analysis in the original table)
Manufacturer
NIPPON STEEL CORPORATION

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV: cannot be calculatedKnown-element contribution; incomplete value; missing C, Mn, Cr, Mo, V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm (Ito–Bessyo): cannot be calculatedKnown-element contribution; incomplete value; missing C, Si, Mn, Cu, Cr, Ni, Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET: cannot be calculatedKnown-element contribution; incomplete value; missing C, Mn, Mo, Cr, Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
P≤ 0.045 (lower limit not stated)
S≤ 0.045 (lower limit not stated)

Applicability and limitations

Historical Nippon Steel wire-rod catalogue EXE203 2008.3, PDF page 9

printed page 14, JIS G3108-2004. Heat analysis (labeled Ladle in the original table).. Manufacturer range data, not guaranteed standard limits or heat-specific measurements; this does not establish supply by Creation Group. Condition: C/Mn not specified in the original table for SGDA/SGDB; Other grades Mn 0.60–0.90 require M suffix agreement; Do not borrow or supplement with zero. The mechanical properties table includes diameter and specimen conditions; these are not flattened as guaranteed values for this batch.

Composition conditions

Verification notes

Grouped tables were expanded in full and checked against original images and notes. Ordinary, residual and conditional elements are kept separate; suffix tables lacking complete base-steel composition are excluded.
WhatsApp Technical enquiry →