← BackMaterial grade directory

SCM420RCH

3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for SCM420RCH →

SCM420RCH · JIS G 3509-1-2021

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Low-alloy steel wire rod for cold heading; ordinary RCH category
Original record status
Original standard verified
Standard edition
JIS G 3509-1:2021
Table / clause
Clause 4/Table 1; Clause 6/Table 2, including the residual Cu note
PDF page references
6、7、8
Unit
Mass fraction (wt%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV:0.4900–0.7067Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2700–0.3825Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3000–0.4263 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.18 ~ 0.23
Si0.15 ~ 0.35
Mn0.6 ~ 0.9
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Cr0.9 ~ 1.2
Cu≤ 0.3 (lower limit not stated)
Mo0.15 ~ 0.25

Applicability and limitations

Based on Table 1/2 of the official Japanese original version of JIS G3509-1:2021, heat analysis mass fraction wt%; This record covers feedstock wire rod; it does not automatically establish the delivery properties or supply of processed WCH wire.. Ordinary RCH, hardenability-guaranteed HRCH, and agreed H1/H2 shall be recorded separately; Chemical ranges for H-class shall follow independent rows in this edition and shall not be automatically widened based on ordinary compositions. Cu≤0.30% for all grades in the table; Do not enter 0 for Mo marked with a dash or for unlisted elements; they must not be intentionally added except as needed to finish steelmaking.; Al addition for grain refinement shall be by agreement. Si is 0.15—0.35% by default; lower limits below 0.15% are adopted by agreement only; This record retains the default range; agreed Si values require separate verification against the actual specified values.. Product analysis deviations shall be verified separately according to the referenced JIS G0321 Table 4; heat limits shall not be treated as product analysis limits. Clause 7.1 applies only when specified by the purchaser. Average ferritic/total decarburized-layer depths: d≤15mm, ≤0.02/0.12mm; 15<d≤25mm, ≤0.02/0.15mm; 25<d≤32mm, ≤0.02/0.20mm; 32<d≤40mm, ≤0.03/0.25mm; 40<d≤50mm, ≤0.03/0.30mm; d>50mm, subject to agreement.. Clause 7.2: Non-metallic inclusion requirements apply only when specified by the purchaser. Use Table 4 of this edition and the corresponding JIS G0555 cleanliness methods; do not automatically equate these with ASTM E45.. Default surface defect depth ≤ 0.10mm; Stricter surface and dimensional accuracy shall be per agreement. Ordinary RCH in this record does not automatically carry the HRCH hardenability guarantee.; Fixed tensile strength and delivery hardness are not specified by the chemical table.

Verification notes

The 2021 official Japanese Table 2, separate composition rows and Cu table note checked; distinct HRCH and ordinary RCH composition ranges retained.

SCM420RCH · JIS G 3509-1-2003

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Material form
Low-alloy steel wire rod for cold heading (RCH/HRCH)
Original record status
Original standard verified
Standard edition
JIS G 3509-1:2003
Table / clause
Main text: Table 1, steel designations and notes 1–2; Table 2, ladle analysis and note (1)/notes 1–3
PDF page references
7、8
Unit
Mass fraction (wt%)
Analysis type
Heat analysis

Carbon-equivalent reference

IIW / CEV:0.4900–0.7067Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2700–0.3825Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3000–0.4263 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.18 ~ 0.23
Si0.15 ~ 0.35
Mn0.6 ~ 0.9
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Cr0.9 ~ 1.2
Mo0.15 ~ 0.25
Cu≤ 0.3 (lower limit not stated)

Applicability and limitations

JIS G 3509-1:2003: main-text Table 1 of the English original lists SCM420RCH, classified as chromium-molybdenum steel. This record covers low-alloy steel wire rod for cold heading. Main-text Table 2 gives heat analysis, mass fraction %. Default Si: 0.15–0.35%. A lower bound below 0.15% requires purchaser-supplier agreement and is not the default. Note 1 to main-text Table 2: impurities for all grades, Cu≤0.30%. Note 2: Al for grain refinement is added only by agreement. Product-analysis deviations apply only by agreement under Table 4 of JIS G 0321. Actual designations in this edition are shown separately from later editions such as 2005/2010/2021; the historical edition does not establish a current standard or actual supply.

Verification notes

2003: Tables 1 and 2 in the body of the original English edition checked row by row; grade SCM420RCH

SCM420RCH · CHINA STEEL CORPORATION · Bars and Wire Rods Product Catalogue 2014-C1 / 7.1.8 JIS G3509-1 (Edition unspecified)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Cold-heading steel
Subcategory
Cold-heading steel
Material form
Bars and wire rod
Original record status
Manufacturer source verified
Document edition
CAT.NO.3-BD-01-2014-C1 (stated on the back cover)
Document title
Bars and Wire Rods Product Catalogue
Table / clause
7.1.8 JIS G3509-1 (Edition unspecified)
PDF page references
16
Unit
Mass fraction (%)
Analysis type
The original catalogue does not explicitly identify the analysis type for this table
Manufacturer
CHINA STEEL CORPORATION

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.4900–0.7067Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2700–0.3825Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3000–0.4263 Envelope of independent element limits from manufacturer data; neither standard guarantee values nor measured heat results CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.18 ~ 0.23
Si0.15 ~ 0.35
Mn0.6 ~ 0.9
P≤ 0.03 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Ni≤ 0.25 (lower limit not stated)
Cr0.9 ~ 1.2
Mo0.15 ~ 0.25
Cu≤ 0.3 (lower limit not stated)

Applicability and limitations

China Steel bar and wire-rod catalogue CAT.NO.3-BD-01-2014-C1, PDF page 16

printed page 14, 7.1.8 JIS G3509-1 (edition not stated). The original catalogue does not explicitly identify the analysis type for this table. Historical manufacturer range data, not guaranteed standard limits or heat-specific measurements; this does not establish supply by Creation Group. Condition, note spanning pages: the Si minimum may be reduced below 0.15 by agreement, and Al may be added for grain refinement; Currently follows the Si range in the main table; no Al limit is inserted without a source.

Composition conditions

Verification notes

Merged cells in all 28 catalogue tables were reconstructed geometrically, with no missing cells. Original images, continuation pages and notes are recorded; disputed conditions are withheld.
WhatsApp Technical enquiry →