SAE1080S
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for SAE1080S →SAE1080S · CHINA STEEL CORPORATION · Bars and Wire Rods Product Catalogue 2014-C1 / 7.1.25 China Steel SAE1080S · Steels for tyre cord
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Carbon steel
- Subcategory
- Carbon steel
- Material form
- Bars and wire rod
- Original record status
- Manufacturer source verified
- Document edition
- CAT.NO.3-BD-01-2014-C1 (stated on the back cover)
- Document title
- Bars and Wire Rods Product Catalogue
- Table / clause
- 7.1.25 China Steel SAE1080S · Steels for tyre cord
- PDF page references
- 28
- Unit
- Mass fraction (%)
- Analysis type
- The original catalogue does not explicitly identify the analysis type for this table
- Manufacturer
- CHINA STEEL CORPORATION
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.81 ~ 0.84 |
| Si | 0.1 ~ 0.3 |
| Mn | 0.45 ~ 0.55 |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Ni | ≤ 0.05 (lower limit not stated) |
| Cr | ≤ 0.05 (lower limit not stated) |
| Cu | ≤ 0.05 (lower limit not stated) |
| Mo | ≤ 0.01 (lower limit not stated) |
| Al | ≤ 0.01 (lower limit not stated) |
| N | ≤ 0.007 (lower limit not stated) |
Applicability and limitations
China Steel Bar and Wire Rod Catalog CAT.NO.3-BD-01-2014-C1, PDF page 28
printed page 26, 7.1.25 China Steel SAE1080S steel for tire wire.. The original catalogue does not explicitly identify the analysis type for this table. Historical manufacturer range data, not guaranteed standard limits or heat-specific measurements; this does not establish supply by Creation Group. Condition: Ceq 0.89–0.93 in the original table uses C+Mn/6; It differs from IIW/Pcm/CET on this site and must not be treated as a separate chemical element or calculated using a formula with the same name..
Composition conditions
- Historical manufacturer 2014-C1 catalogue, bars/wire rod; Where the referenced standard edition is not identified, a year is not borrowed from another catalogue; a catalogue is not upgraded to the official standard text.
- A dash or blank must not be treated as zero. Composition data do not establish completeness or applicability of a formula; mechanical properties and supply require separate verification.
- The original table uses C+Mn/6 for Ceq0.89–0.93; It differs from IIW/Pcm/CET on this site and must not be treated as a separate chemical element or calculated using a formula with the same name..