← BackMaterial grade directory

S43000

13 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for S43000 →

S43000 · SAE J405-1998

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
SAE J405 JUN1998
Table / clause
Table 1, page 2 / page 5, notes 1–7
PDF page references
1、4、5

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.12 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr16.0 ~ 18.0
Ni≤ 0.75 (lower limit not stated)

Applicability and limitations

Based on SAE J405 JUN1998 original Table 1; mass fraction wt%. Note 1: a value without a range or lower limit is a maximum; a dash means unspecified, not zero. Note 5: Cb and Nb denote the same element; verify alloying elements against the corresponding UNS row and additional conditions. Note 4: carbon is generally reported to 0.01%, and low-carbon types to 0.001%; this is reporting precision and does not relax composition limits. Original Table 1 type names may include common names or ASTM-naming footnotes; create search aliases only for explicit same-row correspondences, without implying cross-standard equivalence. 1998 is the actual composition basis; the specified newer edition has not been checked, so consistency between editions is not assumed.

Verification notes

Corresponding UNS rows and table notes in the 1998 original have been checked; this does not verify a newer edition.

S43000 · ASTM A240/A240M-2014

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Ferritic and martensitic stainless steels
Material form
Reference record
Original record status
Original-standard record
Standard edition
ASTM A240/A240M-2014
Table / clause
Table 1 and footnotes A–O
PDF page references
1、5、6

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.12 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr16.0 ~ 18.0
Ni≤ 0.75 (lower limit not stated)

Applicability and limitations

Table 1 ladle composition, mass fraction %; a single value without a range or lower limit is a maximum, and unspecified elements are not filled with zero. Cb and Nb are the same element; where both a formula and a fixed limit apply, use the more restrictive limit. This is a plate, sheet and strip standard; suitability for cold-heading wire and actual supply require separate verification. Clause 4.1 also requires applicable provisions of ASTM A480/A480M. This record shows ladle composition from Table 1; it does not mean that A480 or all product acceptance requirements have been fully checked.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      S43000 · ASTM A 473-2024

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Ferritic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.12 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 1 (lower limit not stated)
      Ni≤ 0.75 (lower limit not stated)
      P≤ 0.04 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S43000 · ASTM A182/A182M-2018

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Ferritic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.12 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 1 (lower limit not stated)
      Ni≤ 0.5 (lower limit not stated)
      P≤ 0.04 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 0.75 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S43000 · ASTM A182/A182M-2025

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Ferritic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.12 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 1 (lower limit not stated)
      Ni≤ 0.5 (lower limit not stated)
      P≤ 0.04 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 0.75 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S43000 · ASTM A276/A276M-2017

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Ferritic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.12 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 1 (lower limit not stated)
      P≤ 0.04 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S43000 · ASTM A276/A276M-2025

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Ferritic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.12 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 1 (lower limit not stated)
      P≤ 0.04 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S43000 · ASTM A473-2018

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Ferritic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.12 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 1 (lower limit not stated)
      Ni≤ 0.75 (lower limit not stated)
      P≤ 0.04 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S43000 · ASTM A473-2026

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Ferritic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.12 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 1 (lower limit not stated)
      Ni≤ 0.75 (lower limit not stated)
      P≤ 0.04 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S43000 · ASTM A479/A479M-2018

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Ferritic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.12 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 1 (lower limit not stated)
      P≤ 0.04 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S43000 · ASTM A479/A479M-2025

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Ferritic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.12 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 1 (lower limit not stated)
      P≤ 0.04 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S43000 · ASTM A815/A815M-2024

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Ferritic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.12 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 1 (lower limit not stated)
      Ni≤ 0.5 (lower limit not stated)
      P≤ 0.04 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S43000 · ASTM A815/A815M-2026

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Ferritic stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.12 (lower limit not stated)
      Cr16 ~ 18
      Mn≤ 1 (lower limit not stated)
      Ni≤ 0.5 (lower limit not stated)
      P≤ 0.04 (lower limit not stated)
      S≤ 0.03 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.