S42030

4 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for S42030 →

S42030 · ASTM A 493-2025

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Original record status
Historical-edition reference
Standard edition
ASTM A493-2009(2013)
Table / clause
Table 1 · Notes A–B
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.3 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr12.0 ~ 14.0
Cu2.0 ~ 3.0
Mo1.0 ~ 3.0

Applicability and limitations

The chemical composition currently shown is transcribed from the original ASTM A493-2009(2013); The original record cites ASTM A 493-2025; that original edition remains unavailable, and differences between editions have not been confirmed. Original text A493−09(Reapproved2013), PDF1 header and PDF2 Table 1

note A–B, wt%. ; Values in Table 1 are maxima unless expressly stated otherwise; Blank elements are unspecified and are not entered as zero. ; This standard covers stainless steel wire and wire rod for cold heading or cold forging; Delivery condition, diameter, surface and actual supply still require confirmation; mechanical-property Table 2 requires separate verification.

Original condition-branch records

Default chemical requirements in Table 1

ElementComposition requirement
C≤ 0.3 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr12.0 ~ 14.0
Cu2.0 ~ 3.0
Mo1.0 ~ 3.0

Verification notes

The chemical composition currently shown is transcribed from the original ASTM A493-2009(2013); The original record cites ASTM A 493-2025; that original edition remains unavailable, and differences between editions have not been confirmed.

S42030 · ASTM A493-2009(2013)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A493-2009(2013)
Table / clause
Table 1 · Notes A–B
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.3 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr12.0 ~ 14.0
Cu2.0 ~ 3.0
Mo1.0 ~ 3.0

Applicability and limitations

Original text A493−09(Reapproved2013), PDF1 header and PDF2 Table 1

note A–B, wt%. ; Values in Table 1 are maxima unless expressly stated otherwise; Blank elements are unspecified and are not entered as zero. ; This standard covers stainless steel wire and wire rod for cold heading or cold forging; Delivery condition, diameter, surface and actual supply still require confirmation; mechanical-property Table 2 requires separate verification.

Original condition-branch records

Default chemical requirements in Table 1

ElementComposition requirement
C≤ 0.3 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr12.0 ~ 14.0
Cu2.0 ~ 3.0
Mo1.0 ~ 3.0

Verification notes

The title page of the official English text and the corresponding row and footnotes in Table 1 were visually checked.

S42030 · ASTM A493-2016

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Original record status
Historical-edition reference
Standard edition
ASTM A493-2009(2013)
Table / clause
Table 1 · Notes A–B
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.3 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr12.0 ~ 14.0
Cu2.0 ~ 3.0
Mo1.0 ~ 3.0

Applicability and limitations

The chemical composition currently shown is transcribed from the original ASTM A493-2009(2013); The original record cites ASTM A493-2016; that original edition remains unavailable, and differences between editions have not been confirmed. Original text A493−09(Reapproved2013), PDF1 header and PDF2 Table 1

note A–B, wt%. ; Values in Table 1 are maxima unless expressly stated otherwise; Blank elements are unspecified and are not entered as zero. ; This standard covers stainless steel wire and wire rod for cold heading or cold forging; Delivery condition, diameter, surface and actual supply still require confirmation; mechanical-property Table 2 requires separate verification.

Original condition-branch records

Default chemical requirements in Table 1

ElementComposition requirement
C≤ 0.3 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr12.0 ~ 14.0
Cu2.0 ~ 3.0
Mo1.0 ~ 3.0

Verification notes

The chemical composition currently shown is transcribed from the original ASTM A493-2009(2013); The original record cites ASTM A493-2016; that original edition remains unavailable, and differences between editions have not been confirmed.

S42030 · ASTM A493-2009(2013)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A493-2009(2013)
Table / clause
Table 1 · Notes A–B
PDF page references
1、2

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.3 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr12.0 ~ 14.0
Cu2.0 ~ 3.0
Mo1.0 ~ 3.0

Applicability and limitations

Original text A493−09(Reapproved2013), PDF1 header and PDF2 Table 1

note A–B, wt%. ; Values in Table 1 are maxima unless expressly stated otherwise; Blank elements are unspecified and are not entered as zero. ; This standard covers stainless steel wire and wire rod for cold heading or cold forging; Delivery condition, diameter, surface and actual supply still require confirmation; mechanical-property Table 2 requires separate verification.

Original condition-branch records

Default chemical requirements in Table 1

ElementComposition requirement
C≤ 0.3 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr12.0 ~ 14.0
Cu2.0 ~ 3.0
Mo1.0 ~ 3.0

Verification notes

The title page of the official English text and the corresponding row and footnotes in Table 1 were visually checked.