S35135 · ASTM A240/A240M-2014

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Original-standard record
Standard edition
ASTM A240/A240M-2014
Table / clause
Table 1 and footnotes A–O
PDF page references
1、4、6

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si0.6 ~ 1.0
Cr20.0 ~ 25.0
Ni30.0 ~ 38.0
Mo4.0 ~ 4.8
Cu≤ 0.75 (lower limit not stated)
Ti0.4 ~ 1

Applicability and limitations

Table 1: heat-analysis composition, mass fraction %. A single value without a stated range or lower bound is a maximum; unspecified elements are not assigned zero. Cb and Nb refer to the same element. Where a formula and fixed limits both apply, use the stricter limit. This is a plate, sheet and strip standard; cold-heading wire applications and actual supply require separate verification. Clause 4.1 also requires compliance with applicable provisions of ASTM A480/A480M. This record displays heat composition from Table 1; it does not establish complete verification of A480 or all product-acceptance requirements. Other elements as printed: Ti 0.40–1.00; see the constraints below for the specific coupled requirements.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat