S35045
2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for S35045 →S35045 · ASTM A240/A240M-2014
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Original record status
- Original-standard record
- Standard edition
- ASTM A240/A240M-2014
- Table / clause
- Table 1 and footnotes A–O
- PDF page references
- 1、4、6
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.06 ~ 0.1 |
| Mn | ≤ 1.5 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Cr | 25.0 ~ 29.0 |
| Ni | 32.0 ~ 37.0 |
| Cu | ≤ 0.75 (lower limit not stated) |
| Al | 0.15 ~ 0.6 |
| Ti | 0.15 ~ 0.6 |
Applicability and limitations
Table 1 gives heat-analysis mass percentages; A single value without a stated range or minimum is a maximum; unspecified elements are not entered as zero. ; Cb and Nb are the same element; Where both a formula and a fixed limit apply, the stricter limit is used. ; This is a plate, sheet and strip standard; cold-heading wire applications and actual supply require separate verification. ; Clause 4.1 also requires compliance with the applicable provisions of ASTM A480/A480M; This record displays the heat composition in Table 1; it does not establish verification of A480 or all product acceptance requirements. ; Other elements in the original table: Al 0.15–0.60 Ti 0.15–0.60; See the limits below for the specific coupled requirements.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat
S35045 · ASTM A312/A312M-2017
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Original record status
- Original-standard record
- Standard edition
- ASTM A312/A312M-2017
- Table / clause
- Table 1, footnotes A–M and clause 7.1
- PDF page references
- 1、2、5、6
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.06 ~ 0.1 |
| Mn | ≤ 1.5 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 1.0 (lower limit not stated) |
| Cr | 25.0 ~ 29.0 |
| Ni | 32.0 ~ 37.0 |
| Ti | 0.15 ~ 0.6 |
| Cu | ≤ 0.75 (lower limit not stated) |
| Al | 0.15 ~ 0.6 |
Applicability and limitations
Table 1 values are mass percentages; a single value is a maximum, and an ellipsis means unspecified—no zero is inferred. Clause 7.1 requires compliance with Table 1; the general requirements of 5.1 and A999/A999M also apply. This review covers only the chemical-composition table. This is an austenitic stainless-steel pipe standard and does not establish cold-heading wire suitability or full product acceptance. Note C: the nitrogen test method is agreed between buyer and seller.
Combined limits
- Combined-element limits