← BackMaterial grade directory

S33228

3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for S33228 →

S33228 · SAE J405-1998

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
SAE J405 JUN1998
Table / clause
Table 1, page 2 / page 5, notes 1–7
PDF page references
1、3、5

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.04 ~ 0.08
Mn≤ 1.0 (lower limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.03 (lower limit not stated)
Cr26.0 ~ 28.0
Ni31.0 ~ 33.0
Ce0.05 ~ 0.1
Nb0.6 ~ 1
Al≤ 0.025 (lower limit not stated)

Applicability and limitations

Based on SAE J405 JUN1998 original Table 1; mass fraction wt%. Note 1: a value without a range or lower limit is a maximum; a dash means unspecified, not zero. Note 5: Cb and Nb denote the same element; verify alloying elements against the corresponding UNS row and additional conditions. Note 4: carbon is generally reported to 0.01%, and low-carbon types to 0.001%; this is reporting precision and does not relax composition limits. Original Table 1 type names may include common names or ASTM-naming footnotes; create search aliases only for explicit same-row correspondences, without implying cross-standard equivalence. 1998 is the actual composition basis; the specified newer edition has not been checked, so consistency between editions is not assumed.

Verification notes

Corresponding UNS rows and table notes in the 1998 original have been checked; this does not verify a newer edition.

S33228 · ASTM A240/A240M-2014

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Original-standard record
Standard edition
ASTM A240/A240M-2014
Table / clause
Table 1 and footnotes A–O
PDF page references
1、3、6

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.04 ~ 0.08
Mn≤ 1.0 (lower limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.3 (lower limit not stated)
Cr26.0 ~ 28.0
Ni31.0 ~ 33.0
Ce0.05 ~ 0.1
Nb0.6 ~ 1
Al≤ 0.025 (lower limit not stated)

Applicability and limitations

Table 1 gives heat-analysis mass percentages; A single value without a stated range or minimum is a maximum; unspecified elements are not entered as zero. ; Cb and Nb are the same element; Where both a formula and a fixed limit apply, the stricter limit is used. ; This is a plate, sheet and strip standard; cold-heading wire applications and actual supply require separate verification. ; Clause 4.1 also requires compliance with the applicable provisions of ASTM A480/A480M; This record displays the heat composition in Table 1; it does not establish verification of A480 or all product acceptance requirements. ; Other elements in the original table: Ce 0.05–0.10 Cb 0.6–1.0 Al 0.025; See the limits below for the specific coupled requirements.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      S33228 · ASTM A312/A312M-2017

      Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

      Material category
      Stainless steel
      Subcategory
      Austenitic stainless steel
      Material form
      Reference record
      Original record status
      Original-standard record
      Standard edition
      ASTM A312/A312M-2017
      Table / clause
      Table 1, footnotes A–M and clause 7.1
      PDF page references
      1、2、5、6

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C0.04 ~ 0.08
      Mn≤ 1.0 (lower limit not stated)
      P≤ 0.02 (lower limit not stated)
      S≤ 0.015 (lower limit not stated)
      Si≤ 0.3 (lower limit not stated)
      Cr26.0 ~ 28.0
      Ni31.0 ~ 33.0
      Nb0.6 ~ 1.0
      Ce0.05 ~ 0.1
      Al≤ 0.025 (lower limit not stated)

      Applicability and limitations

      Table 1 values are mass percentages; a single value is a maximum, and an ellipsis means unspecified—no zero is inferred. Clause 7.1 requires compliance with Table 1; the general requirements of 5.1 and A999/A999M also apply. This review covers only the chemical-composition table. This is an austenitic stainless-steel pipe standard and does not establish cold-heading wire suitability or full product acceptance. Note C: the nitrogen test method is agreed between buyer and seller.

      Combined limits

      Combined-element limits
        WhatsApp Technical enquiry →