← BackMaterial grade directory

S31803

34 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for S31803 →

S31803 · SAE J405-1998

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
SAE J405 JUN1998
Table / clause
Table 1, page 2 / page 5, notes 1–7
PDF page references
1、4、5

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr21.0 ~ 23.0
Ni4.5 ~ 6.5
Mo2.5 ~ 3.5
N0.08 ~ 0.2

Applicability and limitations

Based on SAE J405 JUN1998 original Table 1; mass fraction wt%. Note 1: a value without a range or lower limit is a maximum; a dash means unspecified, not zero. Note 5: Cb and Nb denote the same element; verify alloying elements against the corresponding UNS row and additional conditions. Note 4: carbon is generally reported to 0.01%, and low-carbon types to 0.001%; this is reporting precision and does not relax composition limits. Original Table 1 type names may include common names or ASTM-naming footnotes; create search aliases only for explicit same-row correspondences, without implying cross-standard equivalence. 1998 is the actual composition basis; the specified newer edition has not been checked, so consistency between editions is not assumed.

Verification notes

Composition and table notes were checked using the UNS correspondence in the original 1998 text.

S31803 · SAE J405-2018

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Original record status
Historical-edition reference
Standard edition
SAE J405 JUN1998
Table / clause
Table 1, page 2 / page 5, notes 1–7
PDF page references
1、4、5

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr21.0 ~ 23.0
Ni4.5 ~ 6.5
Mo2.5 ~ 3.5
N0.08 ~ 0.2

Applicability and limitations

Based on SAE J405 JUN1998 original Table 1; mass fraction wt%. Note 1: a value without a range or lower limit is a maximum; a dash means unspecified, not zero. Note 5: Cb and Nb denote the same element; verify alloying elements against the corresponding UNS row and additional conditions. Note 4: carbon is generally reported to 0.01%, and low-carbon types to 0.001%; this is reporting precision and does not relax composition limits. Original Table 1 type names may include common names or ASTM-naming footnotes; create search aliases only for explicit same-row correspondences, without implying cross-standard equivalence. 1998 is the actual composition basis; the specified newer edition has not been checked, so consistency between editions is not assumed.

Verification notes

The current composition is based on the 1998 original. The specified newer edition has not been checked; equivalence between editions is not assumed.

S31803 · ASTM A955/A955M-2020(c)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
ASTM A955/A955M-2020(c)
Table / clause
Table 2 notes A–E; clauses 1.2,1.6,4.1.3/4.1.6,6.1
PDF page references
1、3、4

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr21.0 ~ 23.0
Ni4.5 ~ 6.5
Mo2.5 ~ 3.5
N0.08 ~ 0.2

Applicability and limitations

The composition alloy in this record is S31803

2205. Table 2 gives heat-analysis mass fractions wt%; values other than ranges are maxima. Ellipses indicate no requirement and are not entered as zero. Alloy type UNS and strength grade Grade are recorded separately; 60/75/80 uses the ksi system and 420/520/550 uses the MPa system. The alloy cannot be inferred from the strength grade. The name 2205 can correspond to S31803 or S32205; each must be used under its confirmed UNS, and the two composition ranges must not be combined. This standard concerns concrete reinforcement; applicability as a supplied cold-heading product is not established.

Verification notes

Official English 20c Table 2, footnotes and applicable clauses checked item by item.

S31803 · SAE J405-1998

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
SAE J405 JUN1998
Table / clause
Table 1, page 2 / page 5, notes 1–7
PDF page references
1、4、5

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr21.0 ~ 23.0
Ni4.5 ~ 6.5
Mo2.5 ~ 3.5
N0.08 ~ 0.2

Applicability and limitations

Based on SAE J405 JUN1998 original Table 1; mass fraction wt%. Note 1: a value without a range or lower limit is a maximum; a dash means unspecified, not zero. Note 5: Cb and Nb denote the same element; verify alloying elements against the corresponding UNS row and additional conditions. Note 4: carbon is generally reported to 0.01%, and low-carbon types to 0.001%; this is reporting precision and does not relax composition limits. Original Table 1 type names may include common names or ASTM-naming footnotes; create search aliases only for explicit same-row correspondences, without implying cross-standard equivalence. 1998 is the actual composition basis; the specified newer edition has not been checked, so consistency between editions is not assumed.

Verification notes

Corresponding UNS rows and table notes in the 1998 original have been checked; this does not verify a newer edition.

S31803 · ASTM A240/A240M-2014

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Original record status
Original-standard record
Standard edition
ASTM A240/A240M-2014
Table / clause
Table 1 and footnotes A–O
PDF page references
1、4、6

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr21.0 ~ 23.0
Ni4.5 ~ 6.5
Mo2.5 ~ 3.5
N0.08 ~ 0.2

Applicability and limitations

Table 1 ladle composition, mass fraction %; a single value without a range or lower limit is a maximum, and unspecified elements are not filled with zero. Cb and Nb are the same element; where both a formula and a fixed limit apply, use the more restrictive limit. This is a plate, sheet and strip standard; suitability for cold-heading wire and actual supply require separate verification. Clause 4.1 also requires applicable provisions of ASTM A480/A480M. This record shows ladle composition from Table 1; it does not mean that A480 or all product acceptance requirements have been fully checked.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      S31803 · Walsin Lihwa official website catalog (steel billets and bars; file named 2024, original edition not indicated)

      Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

      Material category
      Stainless steel
      Subcategory
      Stainless steel
      Material form
      Bars
      Original record status
      Manufacturer source verified
      Document edition
      Official website document 2024_Walsin_Catalog_YT-JY-1.pdf; Publication date and edition number not specified on inner pages
      Document title
      Available Stainless Steel Grades & Chemical Composition — For Stainless Steel Billet & Bar
      Table / clause
      Steel grades and chemical composition table
      PDF page references
      7
      Unit
      Percentages as stated in the original table; refer to the source for the specific basis
      Analysis type
      Analysis type not stated
      Manufacturer
      Walsin Lihwa

      Source document

      Carbon-equivalent reference

      Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Si≤ 1.0 (lower limit not stated)
      Mn≤ 2.0 (lower limit not stated)
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Ni4.5 ~ 6.5
      Cr21.0 ~ 23.0
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2

      Applicability and limitations

      Walsin Lihwa official website catalogue, PDF page 7

      printed page 11, row 3; manufacturer composition table %, covering billets and bars, analysis type not stated. The website filename includes 2024, but no edition number was found inside; not a verified edition of the compared standard or our company’s supply guarantee.

      Composition conditions

      Verification notes

      Composition, conditional rows and linked requirements checked cell by cell against the original image; anomalous row 303 on page 10 excluded.

      S31803 · ASME SA-789

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A 314-2025

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A1082/A1082M-2016

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A182/A182M-2018

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A182/A182M-2025

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A240/240M-2018

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A240/A240M-2020

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A270/A270M-2015

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A270/A270M-2024

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A276/A276M-2017

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A276/A276M-2025

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A479/A479M-2018

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A479/A479M-2025

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A511/A511M-2020

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A511/A511M-2025

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A554-2016

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A554-2026

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A789/A789M-2024

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A790/A790M-2024

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A815/A815M-2024

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A815/A815M-2026

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A949/A949M-2001

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A959-2004

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A959-2019

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A988/A988M-2023

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · ASTM A988/A988M-2026

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · Q/RP 006-2018

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Cu≤ 0.5 (lower limit not stated)
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      S31803 · Q/RP 007-2018

      Original-source verification is incomplete; this is not a formal standard reference

      Material category
      Stainless steel
      Subcategory
      Duplex stainless steel
      Material form
      Reference record
      Verification status
      Reference data; original source not verified

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      C≤ 0.03 (lower limit not stated)
      Cr21 ~ 23
      Cu≤ 0.5 (lower limit not stated)
      Mn≤ 2 (lower limit not stated)
      Mo2.5 ~ 3.5
      N0.08 ~ 0.2
      Ni4.5 ~ 6.5
      P≤ 0.03 (lower limit not stated)
      S≤ 0.02 (lower limit not stated)
      Si≤ 1 (lower limit not stated)

      Applicability and limitations

      A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

      WhatsApp Technical enquiry →