S31277
15 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for S31277 →S31277 · ASTM A240/A240M-2014
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Original record status
- Original-standard record
- Standard edition
- ASTM A240/A240M-2014
- Table / clause
- Table 1 and footnotes A–O
- PDF page references
- 1、3、6
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Mn | ≤ 3.0 (lower limit not stated) |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| Cr | 20.5 ~ 23.0 |
| Ni | 26.0 ~ 28.0 |
| Mo | 6.5 ~ 8.0 |
| N | 0.3 ~ 0.4 |
| Cu | 0.5 ~ 1.5 |
Applicability and limitations
Table 1 ladle composition, mass fraction %; a single value without a range or lower limit is a maximum, and unspecified elements are not filled with zero. Cb and Nb are the same element; where both a formula and a fixed limit apply, use the more restrictive limit. This is a plate, sheet and strip standard; suitability for cold-heading wire and actual supply require separate verification. Clause 4.1 also requires applicable provisions of ASTM A480/A480M. This record shows ladle composition from Table 1; it does not mean that A480 or all product acceptance requirements have been fully checked.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat
S31277 · ASTM A312/A312M-2017
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Original record status
- Original-standard record
- Standard edition
- ASTM A312/A312M-2017
- Table / clause
- Table 1, footnotes A–M and clause 7.1
- PDF page references
- 1、2、4、6
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Mn | ≤ 3.0 (lower limit not stated) |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| Cr | 20.5 ~ 23.0 |
| Ni | 26.0 ~ 28.0 |
| Mo | 6.5 ~ 8.0 |
| N | 0.3 ~ 0.4 |
| Cu | 0.5 ~ 1.5 |
Applicability and limitations
Table 1 values are mass percentages; a single value is a maximum, and an ellipsis means unspecified—no zero is inferred. Clause 7.1 requires compliance with Table 1; the general requirements of 5.1 and A999/A999M also apply. This review covers only the chemical-composition table. This is an austenitic stainless-steel pipe standard and does not establish cold-heading wire suitability or full product acceptance. Note C: the nitrogen test method is agreed between buyer and seller.
Combined limits
- Combined-element limits
S31277 · ASME SA-240
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Cr | 20.5 ~ 23 |
| Cu | 0.5 ~ 1.5 |
| Mn | ≤ 3 (lower limit not stated) |
| Mo | 6.5 ~ 8 |
| N | 0.3 ~ 0.4 |
| Ni | 26 ~ 28 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
S31277 · ASTM A213/A213M-2019
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Cr | 20.5 ~ 23 |
| Cu | 0.5 ~ 1.5 |
| Mn | ≤ 3 (lower limit not stated) |
| Mo | 6.5 ~ 8 |
| N | 0.3 ~ 0.4 |
| Ni | 26 ~ 28 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
S31277 · ASTM A213/A213M-2025
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Cr | 20.5 ~ 23 |
| Cu | 0.5 ~ 1.5 |
| Mn | ≤ 3 (lower limit not stated) |
| Mo | 6.5 ~ 8 |
| N | 0.3 ~ 0.4 |
| Ni | 26 ~ 28 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
S31277 · ASTM A240/240M-2018
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Cr | 20.5 ~ 23 |
| Cu | 0.5 ~ 1.5 |
| Mn | ≤ 3 (lower limit not stated) |
| Mo | 6.5 ~ 8 |
| N | 0.3 ~ 0.4 |
| Ni | 26 ~ 28 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
S31277 · ASTM A240/A240M-2020
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Cr | 20.5 ~ 23 |
| Cu | 0.5 ~ 1.5 |
| Mn | ≤ 3 (lower limit not stated) |
| Mo | 6.5 ~ 8 |
| N | 0.3 ~ 0.4 |
| Ni | 26 ~ 28 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
S31277 · ASTM A249/A249M-2004
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Cr | 20.5 ~ 23 |
| Cu | 0.5 ~ 1.5 |
| Mn | ≤ 3 (lower limit not stated) |
| Mo | 6.5 ~ 8 |
| N | 0.3 ~ 0.4 |
| Ni | 26 ~ 28 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
S31277 · ASTM A249/A249M-2018
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Cr | 20.5 ~ 23 |
| Cu | 0.5 ~ 1.5 |
| Mn | ≤ 3 (lower limit not stated) |
| Mo | 6.5 ~ 8 |
| N | 0.3 ~ 0.4 |
| Ni | 26 ~ 28 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
S31277 · ASTM A249/A249M-2024
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Cr | 20.5 ~ 23 |
| Cu | 0.5 ~ 1.5 |
| Mn | ≤ 3 (lower limit not stated) |
| Mo | 6.5 ~ 8 |
| N | 0.3 ~ 0.4 |
| Ni | 26 ~ 28 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
S31277 · ASTM A312/A312M-2025
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Cr | 20.5 ~ 23 |
| Cu | 0.5 ~ 1.5 |
| Mn | ≤ 3 (lower limit not stated) |
| Mo | 6.5 ~ 8 |
| N | 0.3 ~ 0.4 |
| Ni | 26 ~ 28 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
S31277 · ASTM A580/A580M-2018
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Cr | 20.5 ~ 23 |
| Cu | 0.5 ~ 1.5 |
| Mn | ≤ 3 (lower limit not stated) |
| Mo | 6.5 ~ 8 |
| N | 0.3 ~ 0.4 |
| Ni | 26 ~ 28 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
S31277 · ASTM A580/A580M-2023
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Cr | 20.5 ~ 23 |
| Cu | 0.5 ~ 1.5 |
| Mn | ≤ 3 (lower limit not stated) |
| Mo | 6.5 ~ 8 |
| N | 0.3 ~ 0.4 |
| Ni | 26 ~ 28 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
S31277 · ASTM A959-2019
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Cr | 20.5 ~ 23 |
| Cu | 0.5 ~ 1.5 |
| Mn | ≤ 3 (lower limit not stated) |
| Mo | 6.5 ~ 8 |
| N | 0.3 ~ 0.4 |
| Ni | 26 ~ 28 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
S31277 · U.S. standard
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| Cr | 20.5 ~ 23 |
| Cu | 0.5 ~ 1.5 |
| Mn | ≤ 3 (lower limit not stated) |
| Mo | 6.5 ~ 8 |
| N | 0.3 ~ 0.4 |
| Ni | 26 ~ 28 |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.