S31035
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for S31035 →S31035 · ASTM A312/A312M-2017
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Original record status
- Original-standard record
- Standard edition
- ASTM A312/A312M-2017
- Table / clause
- Table 1, footnotes A–M and clause 7.1
- PDF page references
- 1、2、4、6
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.04 ~ 0.1 |
| Mn | ≤ 0.6 (lower limit not stated) |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | ≤ 0.4 (lower limit not stated) |
| Cr | 21.5 ~ 23.5 |
| Ni | 23.5 ~ 26.5 |
| Nb | 0.4 ~ 0.6 |
| N | 0.2 ~ 0.3 |
| Cu | 2.5 ~ 3.5 |
| B | 0.002 ~ 0.008 |
| W | 3 ~ 4 |
| Co | 1 ~ 2 |
Applicability and limitations
Table 1 values are mass percentages; a single value is a maximum, and an ellipsis means unspecified—no zero is inferred. Clause 7.1 requires compliance with Table 1; the general requirements of 5.1 and A999/A999M also apply. This review covers only the chemical-composition table. This is an austenitic stainless-steel pipe standard and does not establish cold-heading wire suitability or full product acceptance. Note C: the nitrogen test method is agreed between buyer and seller.
Combined limits
- Combined-element limits