← BackMaterial grade directory

S31002

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for S31002 →

S31002 · ASTM A312/A312M-2017

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Original-standard record
Standard edition
ASTM A312/A312M-2017
Table / clause
Table 1, footnotes A–M and clause 7.1
PDF page references
1、2、4、6

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.015 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.15 (lower limit not stated)
Cr24.0 ~ 26.0
Ni19.0 ~ 22.0
Mo≤ 0.1 (lower limit not stated)
N≤ 0.1 (lower limit not stated)

Applicability and limitations

Table 1 values are mass percentages; a single value is a maximum, and an ellipsis means unspecified—no zero is inferred. Clause 7.1 requires compliance with Table 1; the general requirements of 5.1 and A999/A999M also apply. This review covers only the chemical-composition table. This is an austenitic stainless-steel pipe standard and does not establish cold-heading wire suitability or full product acceptance. Note C: the nitrogen test method is agreed between buyer and seller.

Combined limits

Combined-element limits
    WhatsApp Technical enquiry →