← BackMaterial grade directory

QZR0.2

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for QZR0.2 →

QZr0.2 · GB/T 5231-2001

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2001
Table / clause
Table 3 and footnotes
PDF page references
1、3、4、5、6、7、8、9、10、11、12、13、14

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Zr0.15 ~ 0.3
Fe≤ 0.05 (lower limit not stated)
Pb≤ 0.01 (lower limit not stated)
Sn≤ 0.05 (lower limit not stated)
Sb≤ 0.005 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Bi≤ 0.002 (lower limit not stated)
S≤ 0.01 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; Under 2.2, elements with specified lower and upper limits are alloying constituents; a single value is a minimum for copper and a maximum for other elements. A dash means unspecified; it is not entered as zero; Cu+Ag and Ni+Co are subject to combined ranges and are not converted into independent element ranges. The balance remains a balance; subtracting independent maxima does not establish a guaranteed range. Total impurities include all relevant impurities; The sum of listed elements is only a necessary condition and cannot replace complete impurity analysis. Product forms in the original document define the applicable wrought-product scope; they do not establish confirmed supply of cold-heading wire or final properties. Cu is the balance, except for QFe2.5 with an explicit Cu minimum and QTe0.5 with a minimum combined Cu+Te+Sn. Note 1: As/Sb/Bi need not be analyzed, but the supplier must guarantee that the specified limits are not exceeded. Total impurities ≤.5%; major alloying elements are not simply added together.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      The official GB/T 5231—2001 tables 1–4 and applicable footnotes were checked row by row against the source. The condition conflict for seven grades whose Fe content is incompatible with non-magnetic requirements is retained; it is not applied automatically.