← BackMaterial grade directory

QSWRCH45K

3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for QSWRCH45K →

QSWRCH45K · Q/320412 ZTG 223—2021

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Cold-heading steel
Subcategory
Cold-heading steel
Material form
Wire rod
Original record status
Manufacturer source verified
Document edition
2021 edition; Published and implemented 2021-05-18; Supersedes 2020 edition
Document title
Hot-rolled cold-heading steel wire rod for automotive fasteners
Table / clause
Table 2
PDF page references
5
Unit
Mass fraction (wt%)
Manufacturer
Zenith Steel Group Co., Ltd.

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.5200–0.6753Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4533–0.5523Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4800–0.5885 Envelope of independent element limits from manufacturer data; neither standard guarantee values nor measured heat results CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.42 ~ 0.48
Si0.1 ~ 0.35
Mn0.6 ~ 0.9
P≤ 0.02 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Al≥ 0.02 (upper limit not stated)
Cr≤ 0.1 (lower limit not stated)
Ni≤ 0.1 (lower limit not stated)
Cu≤ 0.1 (lower limit not stated)
Mo≤ 0.06 (lower limit not stated)

Applicability and limitations

Zhongtian Steel Q/320412 ZTG 223—2021, Table 2, row 2, PDF page 5, cast analysis wt%. Applies to hot-rolled wire rod; specific orders, delivery and supply by Creation Group require separate confirmation.

Composition conditions

Verification notes

Both grade tables and residual-element groups in the publicly available 2021 edition were checked row by row; Verification excludes the watermark color layer in the PDF source document.

QSWRCH45K · Q/320582 JYG19-2023

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Cold-heading steel
Subcategory
Cold-heading steel
Material form
Wire rod
Original record status
Manufacturer source verified
Document edition
2023 Edition; Published 2023-08-25, implemented 2023-09-25; Supersedes 2019 edition
Document title
Hot-rolled wire rod of cold-heading steel for automotive applications
Table / clause
Table 1
PDF page references
6
Unit
Mass fraction (wt%)
Manufacturer
Jiangsu Yonggang Group Co., Ltd.

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.5200–0.6767Known-element contribution; incomplete value; missing Mo, V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4533–0.5383Known-element contribution; incomplete value; missing Mo, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4800–0.5750Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.42 ~ 0.46
Si0.1 ~ 0.3
Mn0.6 ~ 0.9
P≤ 0.015 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)

Applicability and limitations

Yonggang Q/320582 JYG19-2023, Table 1, row 31 (quenching-and-tempering type), PDF page 6, cast analysis wt%; orders, delivery condition and actual supply by Creation Group require separate confirmation.

Composition conditions

Verification notes

2023 public Chinese edition: Table 1 and clause 6.1 checked line by line; the appended English comparison table was not counted again.

QSWRCH45K · Q/320412 ZTG 5024-2023

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Cold-heading steel
Subcategory
Cold-heading steel
Material form
Wire rod
Original record status
Manufacturer source verified
Document edition
2023 Edition; Published and implemented on 2023-06-25; First publication
Document title
Q-series hot-rolled wire rod for cold-heading steel
Table / clause
Table 1
PDF page references
4
Unit
Mass fraction (wt%)
Manufacturer
Zenith Steel Group Co., Ltd.

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.5200–0.7167Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.4533–0.5667Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4800–0.6050 Envelope of independent element limits from manufacturer data; neither standard guarantee values nor measured heat results CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.42 ~ 0.48
Si0.1 ~ 0.35
Mn0.6 ~ 0.9
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Al≥ 0.02 (upper limit not stated)
Cr≤ 0.2 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Mo≤ 0.1 (lower limit not stated)

Applicability and limitations

Zhongtian Steel Q/320412 ZTG 5024-2023, Table 1, row 20 (PDF page 4), cast analysis wt%; hot-rolled wire rod, orders and supply by Creation Group require separate confirmation.

Composition conditions

Verification notes

2023 public edition, Table 1 and residual-element clauses checked line by line; watermark layer excluded.
WhatsApp Technical enquiry →