← BackMaterial grade directory

QSWRCH35K-C

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for QSWRCH35K-C →

QSWRCH35K-C · Q/XG 243-2019

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Cold-heading steel
Material form
Wire rod
Original record status
Original standard verified
Standard edition
Q/XG 243-2019
Table / clause
Table 1, row 10
PDF page references
2
Unit
Mass fraction (wt%)

Carbon-equivalent reference

IIW / CEV:0.4200–0.6167Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.3533–0.4667Known-element contribution; incomplete value; missing V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.3800–0.5050 Independent-element envelope of standard ranges; not measured heat-analysis values CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.32 ~ 0.38
Si0.1 ~ 0.35
Mn0.6 ~ 0.9
P≤ 0.025 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Cr≤ 0.2 (lower limit not stated)
Ni≤ 0.2 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Mo≤ 0.1 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; Q/XG 243-2019 heat analysis; Local PDF, page 2. Check product-analysis tolerances under GB/T 222; Heat-analysis ranges are not directly treated as guaranteed product-analysis ranges. The enterprise standard covers passenger-vehicle cold-heading steel wire rod requiring vehicle-manufacturer approval; it does not establish Creation Group stock availability, customer approval or substitution approval. Table 1, merged “other” cell: each of Cr/Ni/Cu is ≤0.20%, Mo≤0.10%. Clause 5.4: where a higher or enhanced cold-upsetting level is required, C≥0.30% specimens must first be spheroidize-annealed.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      Original Q/XG 243-2019, Table 1 PDF, page 2: rows and merged cells were visually checked