QSn4-3 · GB/T 5231-2001

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2001
Table / clause
Table 3 and footnotes
PDF page references
1、3、4、5、6、7、8、9、10、11、12、13、14

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Table 3 standard condition
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note 2, nonmagnetic applications: tin bronze Fe≤0.020%; QSi3-1 Fe≤0.030%
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
Sn3.5 ~ 4.5
Al≤ 0.002 (lower limit not stated)
Zn2.7 ~ 3.3
Ni≤ 0.2 (lower limit not stated)
Fe≤ 0.05 (lower limit not stated)
Pb≤ 0.02 (lower limit not stated)
P≤ 0.03 (lower limit not stated)

Applicability and limitations

Mass fraction wt%; Under 2.2, elements with specified lower and upper limits are alloying constituents; a single value is a minimum for copper and a maximum for other elements. A dash means unspecified; it is not entered as zero; Cu+Ag and Ni+Co are subject to combined ranges and are not converted into independent element ranges. The balance remains a balance; subtracting independent maxima does not establish a guaranteed range. Total impurities include all relevant impurities; The sum of listed elements is only a necessary condition and cannot replace complete impurity analysis. Product forms in the original document define the applicable wrought-product scope; they do not establish confirmed supply of cold-heading wire or final properties. Cu is the balance, except for QFe2.5 with an explicit Cu minimum and QTe0.5 with a minimum combined Cu+Te+Sn. Note 1: As/Sb/Bi need not be analyzed, but the supplier must guarantee that the specified limits are not exceeded. Note 5: nickel present as an impurity in tin bronze and aluminum bronze is included in copper content; Cu is the balance in this table; no independent Cu limit is invented. Total impurities ≤.2%; major alloying elements are not simply added together.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Original condition-branch records

      Table 3 standard condition

      ElementComposition requirement
      Sn3.5 ~ 4.5
      Al≤ 0.002 (lower limit not stated)
      Zn2.7 ~ 3.3
      Ni≤ 0.2 (lower limit not stated)
      Fe≤ 0.05 (lower limit not stated)
      Pb≤ 0.02 (lower limit not stated)
      P≤ 0.03 (lower limit not stated)

      Note 2, nonmagnetic applications: tin bronze Fe≤0.020%; QSi3-1 Fe≤0.030%

      ElementComposition requirement
      Sn3.5 ~ 4.5
      Al≤ 0.002 (lower limit not stated)
      Zn2.7 ~ 3.3
      Ni≤ 0.2 (lower limit not stated)
      Fe≤ 0.02 (lower limit not stated)
      Pb≤ 0.02 (lower limit not stated)
      P≤ 0.03 (lower limit not stated)

      A condition branch must be selected

      Yes

      Verification notes

      The official GB/T 5231—2001 tables 1–4 and applicable footnotes were checked row by row against the source. The condition conflict for seven grades whose Fe content is incompatible with non-magnetic requirements is retained; it is not applied automatically.

      QSn4-3 · GB/T 5231-2012

      Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

      Material category
      Copper and copper alloys
      Material form
      Reference record
      Original record status
      Original standard verified
      Standard edition
      GB/T 5231-2012
      Table / clause
      Table 4, row 8, designation T50800
      PDF page references
      10
      Unit
      Mass fraction (wt%)

      Carbon-equivalent reference

      IIW / CEV: not directly applicable to this material category
      Pcm (Ito–Bessyo): not directly applicable to this material category
      CET: not directly applicable to this material category

      Composition

      ElementComposition requirement
      Sn3.5 ~ 4.5
      P≤ 0.03 (lower limit not stated)
      Fe≤ 0.05 (lower limit not stated)
      Pb≤ 0.02 (lower limit not stated)
      Al≤ 0.002 (lower limit not stated)
      Zn2.7 ~ 3.3

      Applicability and limitations

      Mass fraction wt%; GB/T 5231-2012, Table 4, row 8, designation T50800; scanned PDF, PDF physical page 10. Cu is balance; dashes mean unspecified and are not replaced with zero. The total of table-listed impurities is ≤0.2%, subject to the applicable table notes. This standard provides the grade-composition basis for wrought copper and copper alloys; actual supply and cold-heading suitability require separate confirmation.

      Combined limits

      Combined-element limits
        Elements requiring measured values from the same heat

          Verification notes

          Scanned original-standard Table 4 checked cell by cell; anomalous cells and table notes are listed separately for review.