QSCM440
3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for QSCM440 →QSCM440 · Q/320412 ZTG 223—2021
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Cold-heading steel
- Subcategory
- Cold-heading steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- 2021 edition; Published and implemented 2021-05-18; Supersedes 2020 edition
- Document title
- Hot-rolled cold-heading steel wire rod for automotive fasteners
- Table / clause
- Table 2
- PDF page references
- 5
- Unit
- Mass fraction (wt%)
- Manufacturer
- Zenith Steel Group Co., Ltd.
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.38 ~ 0.43 |
| Si | 0.15 ~ 0.35 |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| Cr | 0.9 ~ 1.2 |
| Mo | 0.15 ~ 0.3 |
| Al | ≥ 0.02 (upper limit not stated) |
| Ni | ≤ 0.1 (lower limit not stated) |
| Cu | ≤ 0.1 (lower limit not stated) |
Applicability and limitations
Zhongtian Steel Q/320412 ZTG 223—2021, Table 2, row 8, PDF page 5, cast analysis wt%. Applies to hot-rolled wire rod; specific orders, delivery and supply by Creation Group require separate confirmation.
Composition conditions
- Table 2 heat analysis, mass fractions wt%; Upper limits for residual Cr, Ni, Cu, and Mo for Group II shall be supplemented according to Table 3, with priority given to specific provisions within the table.
- Applicable to hot-rolled round wire rod of Φ5.5–25.0mm for automotive fasteners; Wire rod is delivered in the hot-rolled condition.
- A horizontal line indicates that the limit is not listed in the table, which does not equal zero; Measured mechanical-property data in the hot-rolled condition are to be reported for information only; they are not general guaranteed values.
Verification notes
Both grade tables and residual-element groups in the publicly available 2021 edition were checked row by row; Verification excludes the watermark color layer in the PDF source document.QSCM440 · Q/320582 JYG19-2023
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Cold-heading steel
- Subcategory
- Cold-heading steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- 2023 Edition; Published 2023-08-25, implemented 2023-09-25; Supersedes 2019 edition
- Document title
- Hot-rolled wire rod of cold-heading steel for automotive applications
- Table / clause
- Table 1
- PDF page references
- 6
- Unit
- Mass fraction (wt%)
- Manufacturer
- Jiangsu Yonggang Group Co., Ltd.
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.38 ~ 0.42 |
| Si | 0.15 ~ 0.3 |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.015 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Cr | 0.9 ~ 1.1 |
| Mo | 0.15 ~ 0.3 |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Yonggang Q/320582 JYG19-2023, Table 1, row 37 (quenching-and-tempering type), PDF page 6, cast analysis wt%; orders, delivery condition and actual supply by Creation Group require separate confirmation.
Composition conditions
- Table 1 heat analysis, mass fractions wt%; Dashes in the table do not mean zero..
- Residual Ni and Cu mass fractions are each ≤0.20% per Clause 6.1.3; Cr in the table shall be according to the corresponding grade.
- Footnote a: Al in the table refers to total aluminum; If acid-soluble aluminum Alₛ is determined, then Alₛ≥0.015%..
- Applies to hot-rolled wire rod for automotive fasteners, supplied in the hot-rolled condition.; Annealing and other delivery conditions must be specified in the contract.
Verification notes
2023 public Chinese edition: Table 1 and clause 6.1 checked line by line; the appended English comparison table was not counted again.QSCM440 · Q/320412 ZTG 5024-2023
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Cold-heading steel
- Subcategory
- Cold-heading steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- 2023 Edition; Published and implemented on 2023-06-25; First publication
- Document title
- Q-series hot-rolled wire rod for cold-heading steel
- Table / clause
- Table 1
- PDF page references
- 5
- Unit
- Mass fraction (wt%)
- Manufacturer
- Zenith Steel Group Co., Ltd.
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.38 ~ 0.43 |
| Si | 0.15 ~ 0.35 |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 0.9 ~ 1.2 |
| Mo | 0.15 ~ 0.3 |
| Al | ≥ 0.02 (upper limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Zhongtian Steel Q/320412 ZTG 5024-2023, Table 1, row 37 (PDF page 5), cast analysis wt%; hot-rolled wire rod, orders and supply by Creation Group require separate confirmation.
Composition conditions
- Table 1 cast analysis in mass percent wt%; table dashes are not zero.
- Clause 6.1.3: residual Cr, Ni and Cu each ≤0.20%, Mo≤0.10%; grade-specific table limits take precedence.
- The source specifies hot-rolled delivery of wire rod and calls only for reporting measured mechanical-property data; those properties are not delivery acceptance criteria.