QML20MNTIB-C
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for QML20MNTIB-C →QML20MnTiB-C · Q/XG 243-2019
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Boron steels
- Material form
- Wire rod
- Original record status
- Original standard verified
- Standard edition
- Q/XG 243-2019
- Table / clause
- Table 2, row 5
- PDF page references
- 2
- Unit
- Mass fraction (wt%)
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | 0.19 ~ 0.24 |
| Si | ≤ 0.3 (lower limit not stated) |
| Mn | 1.3 ~ 1.6 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.02 (lower limit not stated) |
| B | 0.001 ~ 0.0035 |
| Al | ≥ 0.02 (upper limit not stated) |
| Cr | ≤ 0.2 (lower limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
| Mo | ≤ 0.15 (lower limit not stated) |
| Ti | 0.04 ~ 0.1 |
Applicability and limitations
Mass fraction wt%; Q/XG 243-2019 heat analysis; Local PDF, page 2. Check product-analysis tolerances under GB/T 222; Heat-analysis ranges are not directly treated as guaranteed product-analysis ranges. The enterprise standard covers passenger-vehicle cold-heading steel wire rod requiring vehicle-manufacturer approval; it does not establish Creation Group stock availability, customer approval or substitution approval.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat