- Material category
- Copper and copper alloys
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 5231-2001
- Table / clause
- Table 3 and footnotes
- PDF page references
- 1、3、4、5、6、7、8、9、10、11、12、13、14
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Cr | 0.6 ~ 1.2 |
| Si | ≤ 0.1 (lower limit not stated) |
| Fe | ≤ 0.1 (lower limit not stated) |
| Pb | ≤ 0.05 (lower limit not stated) |
Applicability and limitations
Mass fraction wt%; Under 2.2, elements with specified lower and upper limits are alloying constituents; a single value is a minimum for copper and a maximum for other elements. A dash means unspecified; it is not entered as zero; Cu+Ag and Ni+Co are subject to combined ranges and are not converted into independent element ranges. The balance remains a balance; subtracting independent maxima does not establish a guaranteed range. Total impurities include all relevant impurities; The sum of listed elements is only a necessary condition and cannot replace complete impurity analysis. Product forms in the original document define the applicable wrought-product scope; they do not establish confirmed supply of cold-heading wire or final properties. Cu is the balance, except for QFe2.5 with an explicit Cu minimum and QTe0.5 with a minimum combined Cu+Te+Sn. Note 1: As/Sb/Bi need not be analyzed, but the supplier must guarantee that the specified limits are not exceeded. Note 6: Cu and the listed elements must total ≥99.5%; A balance element cannot be used to derive a guaranteed interval from independent limits.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat