QAl10-4-4-1 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 4, row 32, designation T61790
PDF page references
10
Unit
Mass fraction (wt%)

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al8.5 ~ 11.0
Fe3.0 ~ 5.0
Ni3.0 ~ 5.0
Mn0.5 ~ 2.0

Applicability and limitations

Mass fraction wt%; GB/T 5231-2012, Table 4, row 32, designation T61790; scanned PDF, PDF physical page 10. Cu is balance; dashes mean unspecified and are not replaced with zero. The total of table-listed impurities is ≤0.8%, subject to the applicable table notes. This standard provides the grade-composition basis for wrought copper and copper alloys; actual supply and cold-heading suitability require separate confirmation. Note a to Table 4: analysis of As, Sb and Bi may be omitted, but the supplier must ensure that their contents do not exceed the table limits.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      Scanned original-standard Table 4 checked cell by cell; anomalous cells and table notes are listed separately for review.
      WhatsApp Technical enquiry →