Q620MD

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for Q620MD →

Q620MD · GB/T 1591-2018

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
High-strength low-alloy structural steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 1591-2018
Table / clause
Table 5 · Footnotes
PDF page references
12、12
Unit
Mass fraction (wt%)
Analysis type
Heat analysis, not product analysis
Original composition-element notation and analysis basis
Al
Original element symbol
Als
Subscript in the original source
s
Additional source notes
Acid-soluble aluminum in the original table
PDF page references
12

When the original analysis designations differ, or a record leaves them unspecified, comparability or a match cannot be concluded directly. Subscripts not explained by the source are not expanded here.

Carbon-equivalent reference

IIW / CEV:0.0000–1.0040 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved; coupled-element constraints require separate checks, and the entire envelope is not guaranteed to be realizable CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0000–0.4853 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved; coupled-element constraints require separate checks, and the entire envelope is not guaranteed to be realizable Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0000–0.5800 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved; coupled-element constraints require separate checks, and the entire envelope is not guaranteed to be realizable CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C≤ 0.18 (lower limit not stated)
Si≤ 0.6 (lower limit not stated)
Mn≤ 2.6 (lower limit not stated)
P≤ 0.03 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Nb0.01 ~ 0.11
V0.01 ~ 0.12
Ti0.006 ~ 0.05
Cr≤ 1 (lower limit not stated)
Ni≤ 0.8 (lower limit not stated)
Cu≤ 0.8 (lower limit not stated)
Mo≤ 0.3 (lower limit not stated)
N≤ 0.025 (lower limit not stated)
Als≥ 0.015 (upper limit not stated)
B≤ 0.004 (lower limit not stated)

Applicability and limitations

At least one of Al, Nb, V and Ti must be present; When added individually or in combination, at least one element must reach its tabulated minimum; all four elements are not required to meet the listed minima. For sections and bars, the P and S maxima may each be increased by 0.005%. Ti may reach a maximum of 0.20%. Total aluminum Alt may replace acid-soluble aluminum Als, with a Alt minimum of 0.020%; Where grain-refining elements such as Nb, V or Ti are added and meet the stated minima, the aluminum minimum does not apply. In the original table, Als refers to acid-soluble aluminum and Alt refers to total aluminum; analysis types cannot be directly compared or mixed.; Using Alt as a substitute, or waiving the aluminum lower limit under the microalloying conditions, requires checking the original note and measured test report.. At least one of Al/Nb/V/Ti must reach the corresponding lower limit.; It is not required for all elements to simultaneously reach the lower limit; elements not reported shall not be treated as 0.. This batch only verifies the composition table and conditions.; The calculated independent-element envelope does not establish compliance with the CEV/Pcm upper limits in Tables 4/6 for the applicable thickness/delivery condition; the actual heat and corresponding table must still be checked.. Retain normalized/normalizing-rolled condition N and thermomechanically rolled condition M separately; a shared steel grade does not make the delivery conditions interchangeable..

Combined limits

Grain-refining element combination options
Al
0.015
Nb
0.01
V
0.01
Ti
0.006
Conditional composition lower limit
  • Al
  • Nb
  • V
  • Ti
Product-form exception
P
0.005
S
0.005
C
0.02
Conditional Ti upper limit
0.2

Verification notes

Missing-data rows and footnotes spanning pages in the original table were checked; other verified rows of the same edition were reused; Al analysis designations and delivery condition are retained.