Q550MC
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for Q550MC →Q550MC · GB/T 1591-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- High-strength low-alloy structural steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 1591-2018
- Table / clause
- Table 5 · Footnotes
- PDF page references
- 12、12
- Unit
- Mass fraction (wt%)
- Analysis type
- Heat analysis, not product analysis
Original composition-element notation and analysis basis
- Al
- Original element symbol
- Als
- Subscript in the original source
- s
- Additional source notes
- Acid-soluble aluminum in the original table
- PDF page references
- 12
When the original analysis designations differ, or a record leaves them unspecified, comparability or a match cannot be concluded directly. Subscripts not explained by the source are not expanded here.
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.18 (lower limit not stated) |
| Si | ≤ 0.6 (lower limit not stated) |
| Mn | ≤ 2 (lower limit not stated) |
| P | ≤ 0.03 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Nb | 0.01 ~ 0.11 |
| V | 0.01 ~ 0.12 |
| Ti | 0.006 ~ 0.05 |
| Cr | ≤ 0.8 (lower limit not stated) |
| Ni | ≤ 0.8 (lower limit not stated) |
| Cu | ≤ 0.8 (lower limit not stated) |
| Mo | ≤ 0.3 (lower limit not stated) |
| N | ≤ 0.015 (lower limit not stated) |
| Als | ≥ 0.015 (upper limit not stated) |
| B | ≤ 0.004 (lower limit not stated) |
Applicability and limitations
At least one of Al, Nb, V and Ti must be present; When added individually or in combination, at least one element must reach its tabulated minimum; all four elements are not required to meet the listed minima. For sections and bars, the P and S maxima may each be increased by 0.005%. Ti may reach a maximum of 0.20%. Total aluminum Alt may replace acid-soluble aluminum Als, with a Alt minimum of 0.020%; Where grain-refining elements such as Nb, V or Ti are added and meet the stated minima, the aluminum minimum does not apply. In the original table, Als refers to acid-soluble aluminum and Alt refers to total aluminum; analysis types cannot be directly compared or mixed.; Using Alt as a substitute, or waiving the aluminum lower limit under the microalloying conditions, requires checking the original note and measured test report.. At least one of Al/Nb/V/Ti must reach the corresponding lower limit.; It is not required for all elements to simultaneously reach the lower limit; elements not reported shall not be treated as 0.. This batch only verifies the composition table and conditions.; The calculated independent-element envelope does not establish compliance with the CEV/Pcm upper limits in Tables 4/6 for the applicable thickness/delivery condition; the actual heat and corresponding table must still be checked.. Retain normalized/normalizing-rolled condition N and thermomechanically rolled condition M separately; a shared steel grade does not make the delivery conditions interchangeable..
Combined limits
- Grain-refining element combination options
- Al
- 0.015
- Nb
- 0.01
- V
- 0.01
- Ti
- 0.006
- Conditional composition lower limit
- Al
- Nb
- V
- Ti
- Product-form exception
- P
- 0.005
- S
- 0.005
- C
- 0.02
- Conditional Ti upper limit
- 0.2