← BackMaterial grade directory

Q550E

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for Q550E →

Q550E · GB/T 1591-2008

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
High-strength low-alloy structural steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 1591-2008
Table / clause
Table 1 · continued table · Notes a/b; 6.1.1–6.1.7

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Cr/Ni/Cu are residual elements, each ≤0.30%; Al in the table is acid-soluble aluminum Al(s)
IIW / CEV:0.0000–0.6973 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0000–0.3870 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0000–0.4475 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Cr/Ni/Cu are residual elements, each ≤0.30%; Based on total aluminum Al(t)≥0.020%
IIW / CEV:0.0000–0.6973 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0000–0.3870 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0000–0.4475 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Cr/Ni/Cu is intentionally added; the maximum in Table 1 is used; A separate agreement requires individual confirmation; Al in the table is acid-soluble aluminum Al(s)
IIW / CEV:0.0000–0.8640 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0000–0.4453 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0000–0.5100 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Cr/Ni/Cu is intentionally added; the maximum in Table 1 is used; A separate agreement requires individual confirmation; Based on total aluminum Al(t)≥0.020%
IIW / CEV:0.0000–0.8640 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.0000–0.4453 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.0000–0.5100 Independent-element envelope of standard ranges, not measured heat results; ordering or conditional requirements remain unresolved CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.18 (lower limit not stated)
Si≤ 0.6 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
Nb≤ 0.11 (lower limit not stated)
V≤ 0.12 (lower limit not stated)
Ti≤ 0.2 (lower limit not stated)
Cr≤ 0.8 (lower limit not stated)
Ni≤ 0.8 (lower limit not stated)
Cu≤ 0.8 (lower limit not stated)
N≤ 0.015 (lower limit not stated)
Mo≤ 0.3 (lower limit not stated)
B≤ 0.004 (lower limit not stated)
P≤ 0.025 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Al≥ 0.015 (upper limit not stated)

Applicability and limitations

Heat analysis, mass fractions wt%; Retain the identity of the 2008 edition; do not apply the 2018 edition.. ; When grain refining elements need to be added per 6.1.2, at least one of Al/Nb/V/Ti must be contained and specified in the quality certificate.; This clause does not provide mandatory general lower limits for all elements.. ; 6.1.4 When nitrogen-fixing alloying elements such as Al/Nb/V/Ti are added, N is not restricted, but the nitrogen-fixing elements must be specified.; If this condition is not selected, the N upper limit listed in the table is the default.. ; Table 1, Note a: For sections/bars, the P and S limits may each increase by 0.005%; the upper limit for quality class A may be 0.045%.; Cannot be used for other products.. ; Table 1 Note b: When grain refining elements are added in combination, Nb+V+Ti≤0.22% and Mo+Cr≤0.30%.; The individual-element upper limits cannot all be taken simultaneously.. ; Clause 6.1.6: RE is calculated as an addition of 0.02–0.20% of the molten-steel weight, not as guaranteed finished-product composition..

Combined limits

Product-form exception
P
0.005
S
0.005
Class A product-form upper limit
Not stated
Element-sum limits
    Conditional combined limit
    • Elements concerned
      • Nb
      • V
      • Ti
      Upper limit
      0.22
    • Elements concerned
      • Mo
      • Cr
      Upper limit
      0.3
    Nitrogen-fixing exception conditions
    Yes

    Original condition-branch records

    Cr/Ni/Cu are residual elements, each ≤0.30%; Al in the table is acid-soluble aluminum Al(s)

    ElementComposition requirement
    C≤ 0.18 (lower limit not stated)
    Si≤ 0.6 (lower limit not stated)
    Mn≤ 2.0 (lower limit not stated)
    Nb≤ 0.11 (lower limit not stated)
    V≤ 0.12 (lower limit not stated)
    Ti≤ 0.2 (lower limit not stated)
    Cr≤ 0.3 (lower limit not stated)
    Ni≤ 0.3 (lower limit not stated)
    Cu≤ 0.3 (lower limit not stated)
    N≤ 0.015 (lower limit not stated)
    Mo≤ 0.3 (lower limit not stated)
    B≤ 0.004 (lower limit not stated)
    P≤ 0.025 (lower limit not stated)
    S≤ 0.02 (lower limit not stated)
    Al≥ 0.015 (upper limit not stated)

    Cr/Ni/Cu are residual elements, each ≤0.30%; Based on total aluminum Al(t)≥0.020%

    ElementComposition requirement
    C≤ 0.18 (lower limit not stated)
    Si≤ 0.6 (lower limit not stated)
    Mn≤ 2.0 (lower limit not stated)
    Nb≤ 0.11 (lower limit not stated)
    V≤ 0.12 (lower limit not stated)
    Ti≤ 0.2 (lower limit not stated)
    Cr≤ 0.3 (lower limit not stated)
    Ni≤ 0.3 (lower limit not stated)
    Cu≤ 0.3 (lower limit not stated)
    N≤ 0.015 (lower limit not stated)
    Mo≤ 0.3 (lower limit not stated)
    B≤ 0.004 (lower limit not stated)
    P≤ 0.025 (lower limit not stated)
    S≤ 0.02 (lower limit not stated)
    Al≥ 0.02 (upper limit not stated)

    Cr/Ni/Cu is intentionally added; the maximum in Table 1 is used; A separate agreement requires individual confirmation; Al in the table is acid-soluble aluminum Al(s)

    ElementComposition requirement
    C≤ 0.18 (lower limit not stated)
    Si≤ 0.6 (lower limit not stated)
    Mn≤ 2.0 (lower limit not stated)
    Nb≤ 0.11 (lower limit not stated)
    V≤ 0.12 (lower limit not stated)
    Ti≤ 0.2 (lower limit not stated)
    Cr≤ 0.8 (lower limit not stated)
    Ni≤ 0.8 (lower limit not stated)
    Cu≤ 0.8 (lower limit not stated)
    N≤ 0.015 (lower limit not stated)
    Mo≤ 0.3 (lower limit not stated)
    B≤ 0.004 (lower limit not stated)
    P≤ 0.025 (lower limit not stated)
    S≤ 0.02 (lower limit not stated)
    Al≥ 0.015 (upper limit not stated)

    Cr/Ni/Cu is intentionally added; the maximum in Table 1 is used; A separate agreement requires individual confirmation; Based on total aluminum Al(t)≥0.020%

    ElementComposition requirement
    C≤ 0.18 (lower limit not stated)
    Si≤ 0.6 (lower limit not stated)
    Mn≤ 2.0 (lower limit not stated)
    Nb≤ 0.11 (lower limit not stated)
    V≤ 0.12 (lower limit not stated)
    Ti≤ 0.2 (lower limit not stated)
    Cr≤ 0.8 (lower limit not stated)
    Ni≤ 0.8 (lower limit not stated)
    Cu≤ 0.8 (lower limit not stated)
    N≤ 0.015 (lower limit not stated)
    Mo≤ 0.3 (lower limit not stated)
    B≤ 0.004 (lower limit not stated)
    P≤ 0.025 (lower limit not stated)
    S≤ 0.02 (lower limit not stated)
    Al≥ 0.02 (upper limit not stated)

    A condition branch must be selected

    Yes

    Verification notes

    Original text of Table 1, notes a/b and the applicability conditions in Clause 6.1 checked
    WhatsApp Technical enquiry →